Based on the measured stress-strain curves and thermo-physical data of 25Cr2Ni4MoV steel, a FEM model of void closure in heavy forging process was established through ABAQUS software. The void closure behaviors under different hot plasticity conditions have been investigated. The FEM results showed three distinct stages during the void closure. The voids with the same position in a cylindrical specimen close up at a similar height reduction ratio (ΔH/H0) around 25\% at different temperatures, which indicates that the void closure is not sensitive to the deformation temperature. On basis of the FEM results, a physical-simulated experiment for void bonding process has been performed through compression tests on a hollow cylindrical specimens, with deformation temperatures ranging from 900 ℃ to 1200 ℃, ΔH/H0 from 25\% to 45\% and a constant strain rate 0.01 s-1. The experimental results have shown that the ΔH/H0 for the void completely bonded at 1200, 1100 and 1000℃ are all about 35%, but increases to 45\% when the deformation temperature decreased to 900℃, which confirms that void bonding is a diffusion controlled process. Through the experimental results, it can be further demonstrated the high temperature combined with severe deformation can enhance the ability of atoms transition and decrease the micro-gap between contacted surfaces. Finally, the influencing factors on the bonding efficiency were investigated through SEM observation on the fractured surface of the tensile specimen with internal closed void.
LI Dian-Zhong
. STUDY ON VOID HEALING BEHAVIOR DURING FORGING PROCESS FOR 25Cr2Ni4MoV STEEL[J]. Acta Metall Sin, 2011
, 47(7)
: 946
-953
.
DOI: 10.3724/SP.J.1037.2011.00157
[1] National Development and Reform Commission. Nuclear Power Medium– and Long–term Development Program 2005—2020, May, 2007
(国家发展和改革委员会. 核电中长期发展规划(2005-2020年). 2007年5月)
[2] Sigworth G K, Wang C M. Metall Trans, 1993; 24B: 349
[3] Lu Y. The Theory and Process of Forging. Beijing: China Machine Press, 1991: 321
(吕炎. 锻压成形理论与工艺. 北京: 机械工业出版社, 1991: 321)
[4] Kallstrom R. Scand J Metall, 1983; 12: 121
[5] Cook P M. J Iron Steel Inst Jpn, 1959; 4: 250
[6] Wang L G, Huang Y, Liu Z B. J Plast Eng, 2002; 9(2): 28
(王雷刚, 黄瑶, 刘助柏. 塑性工程学报, 2002; 9(2): 28)
[7] Park C Y, Yang D Y. J Mater Process Technol, 1996; 57: 129
[8] Wang A, Thomson P F, Hodgson P D. J Mater Process Technol, 1996; 60: 95
[9] Chen K, Yang Y T, Liu K J, Shao G J. Adv Mater Res, 2010; 11: 3079
[10] Zhang X X, Cui Z S. Appl Math Mech (Engl Ed), 2009; 30: 631
[11] Zhu M. J Beijing Inst Technol, 1990; 10(2): 58
(朱明. 北京理工大学学报, 1990; 10(2): 58)
[12] Cui Z S, Ren G S, Xu B Y, Xu C G, Liu G H. J Tsinghua Univ (Sci Technol), 2003; 43: 227
(崔振山, 任广升, 徐秉业, 徐春国, 刘桂华. 清华大学学报(自然科学版), 2003; 43: 227)
[13] Lee Y S, Kwon Y C, Kwon Y N, Lee J H, Lee S W, Kim N S. Adv Mater Res, 2007; 26: 69
[14] Yuan C L, Zhong Y X, Ma Q X. Sci China, 2002; 45E: 531
[15] Petrov A I, Razuvaeva M V. Phys Solid State, 2005; 47: 880
[16] Schleisiek K, Lechler T, Schafer L, Weimar P. J Nucl Mater, 2000; 283: 1196
[17] Huang H G, Du F S, Xu Z Q. J Iron Steel Res, 2007; 19(11): 55
(黄华贵, 杜凤山, 许志强. 钢铁研究学报, 2007; 19(11): 55)
[18] Liu L J, Cui Z S. J Plast Eng, 2010; 17(1): 1
(刘丽娟, 崔振山. 塑性工程学报, 2010; 17(1): 1)
[19] Park C Y, Yang D Y. J Mater Process Technol, 1997; 72: 32
[20] Tanaka M, Ono S, Tsuneno M, Iwadate T. Adv Technol Plast, 1987; 2: 1035
[21] Morihiko N, Ichiro T, Hirosh U. J Mater Process Technol, 2006; 177: 521
[22] Kakimoto H, Arikawa T, Takahashi Y, Tanaka T, Imaida Y. J Mater Process Technol, 2010; 210: 415