CORROSION FATIGUE OF NUCLEAR--GRADE STAINLESS STEEL IN
HIGH TEMPERATURE WATER AND ITS ENVIRONMENTAL FATIGUE DESIGN MODEL

  • WU Xin-Jiang
Expand
  • 1) State Key Laboratory for Corrosion and Protection, Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016
    2) Liaoning Key Laboratory for Safety and Assessment Technique of Nuclear Material, Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016

Received date: 2011-03-23

  Revised date: 2011-04-11

  Online published: 2011-07-11

Supported by

Supported by National Basic Research Program of China (No.2011CB610506) and National Science and Technology Major Project (No.2011ZX06004-009)

Abstract

The high safety of light water reactor nuclear power plants (NPPs) requires very strict design standard and service property of pressure boundary components materials. The service degradation and life assessment of the components materials primarily depend on the understanding of environmentally assisted failure mechanism, accumulation of service property data and construction of evaluation models. Currently domestic NPPs are relying on foreign design, operation and life assessment standards. However, recent experimental data indicate that even the ASME design fatigue code may be deficient in safety margin under certain conditions of loading and environment. In the present work, based on the corrosion fatigue tests in simulated NPPs' high temperature pressurized water, the corrosion fatigue behavior and environmentally assisted failure mechanism of domestic nuclear-grade stainless steel have been investigated. The factors affecting fatigue life of nuclear grade stainless steel in high temperature water were evaluated. A design fatigue model was constructed by taking environmental degradation effects into account and the corresponding design curves were given for the convenience of engineering applications.

Cite this article

WU Xin-Jiang . CORROSION FATIGUE OF NUCLEAR--GRADE STAINLESS STEEL IN
HIGH TEMPERATURE WATER AND ITS ENVIRONMENTAL FATIGUE DESIGN MODEL[J]. Acta Metall Sin, 2011
, 47(7) : 790 -796 . DOI: 10.3724/SP.J.1037.2011.00162

References

[1] Cahn R W, Haasen P, Kramer E J. Mater Sci Technol, 1994: 10B: 38

[2] Wu X Q, Han E H, Ke W, Katada Y. Nucl Eng Des, 2007; 237: 1452

[3] Wu X Q, Kataday Y. Corros Sci, 2005; 47: 1415

[4] Raman S G S, Kitsunai Y. Eng Fail Anal, 2004; 11: 293

[5] Chopra O K, Shack W J. ASME PVP, 2003; 453: 71

[6] Chopra O K, Shack W J. Nucl Eng Des, 1998; 184: 49

[7] Higuchi M, Iida K, Asada Y. In: Van Der Sluys WA, Piascik R S, Zauierucha R, eds., Effects of Strain Rate Change on Fatigue Life of Carbon Steel in High–Temperature Water, ASTM STP 1298, Philadelphia: American Society for Testing and Materials, 1997: 216

[8] H¨anninen H, Cullen W, Kemppainen M. Corrosion, 1990; 46: 563

[9] Kuniya J, Anzai H, Masaoka I. Corrosion, 1992; 48: 419

[10] Atkinson J D, Yu J. Fatigue Fract Eng Mater Struct, 1997; 20: 1

[11] Chopra O K, Shack W J. J Pressure Vessel Technol Trans ASME, 1999; 121: 49

[12] Ford F P. Corrosion, 1996; 52: 375

[13] Maiya P S. J Pressure Vessel Technol Trans ASME, 1987; 109: 116

[14] Xu S, Wu X Q, Han E H, Ke W, Katada Y. Mater Sci Eng, 2008; A49: 16

[15] Laird C, Smith G C. Philo Mag, 1962; 8: 847

[16] Laird C, Finney J M, Wilsdorf D K. Mater Sci Eng, 1981; 50: 127

[17] Langer B F. ASME J Basic Eng, 1962; 84: 389
Outlines

/