Abstract

The corrosion behaviors of Hastelloy C276 alloy and Hastelloy N alloy in 80%CaCl2+20%CaF2 (mass fraction) molten salt were investigated by XRD, OM, SEM and EDS. The results show that intergranular corrosion takes place in the two alloys, and the form of intergranular corrosion is a type of selective corrosion, i.e., the desolutions of Cr and Mo occur along the grain boundary. The corrosion rates of the two alloys decelerate with the increases of corrosion time because of the hindering effect of corrosion products on the element diffusion, and the relationship of mass loss ($C$) and corrosion time (t) can be described by formula of C=Ktn.

Cite this article

PENG Hai-Jian , JIN Jun , LI De-Fu , HU Cha , XU Xiao-Jing , MAO Bai-Beng . CORROSION BEHAVIORS OF Ni-Cr-Mo CORROSION RESISTENCE ALLOYS IN CaCl2-CaF2 MOLTEN SALT[J]. Acta Metall Sin, 2011 , 47(9) : 1195 -1199 . DOI: 10.3724/SP.J.1037.2011.00108

References

[1] Bai X D. Nuclear Material Chemistry. Beijing: Chemical Industry Press, 2007: 513

(白新德. 核材料化学. 北京: 化学工业出版社, 2007: 513)

[2] Xu W J, Ma C L, Sha R L. Corrosion and Protection in Nuclear Industry. Beijing: Chemical Industry Press, 1993: 147

(许维钧, 马春来, 沙仁礼. 核工业中的腐蚀与防护. 北京: 化学工业出版社, 1993: 147)

[3] Li Y S, Wang F G, Niu Y. Rare Met Mater Eng, 2001; 30: 376

(李远士, 王富岗, 牛炎. 稀有金属材料与工程. 2001; 30: 376)

[4] Lee Y Y, Mcnallan M J. Metall Trans, 1987; 18A: 1099

[5] Zahs A, Spiegel M, Grabke H J. Corros Sci, 2000; 42: 1093

[6] Juergen G G, Evan H G. Clinical Mater, 1989; 4: 225

[7] Rebak R B. Adv Mater Proc, 2000; 157: 37

[8] Wang F P, KangWL, Jing H M. Fundamentals of Electrochemical Corrosion, Methods and Applications. Beijing: Chemical Industry Press, 2008: 15

(王凤平, 康万利, 敬和民. 腐蚀电化学原理、方法及应用. 北京: 化学工业出版社, 2008: 15)

[9] Chinese Cankerous and Protection Society. Handbook of Metal Corrosion. Shanghai: Shanghai Scientific and Technical Publishers, 1987: 132

(中国腐蚀与防护学会. 金属腐蚀手册. 上海: 上海科学技术出版社, 1987: 132)
Outlines

/

〈 〉