EFFECT OF HYDROSTATIC PRESSURE ON THE CORROSION BEHAVIORS OF TWO LOW ALLOY STEELS

  • LIU Jie ,
  • LI Xiang-Bei ,
  • YU Jia
Expand
  • 1. College of Chemistry and Chemical Engineering, Ocean University of China, Qingdao 266100
    2. Science and Technology on Marine Corrosion and Protection Laboratory, Luoyang Ship Material Research Institute (LSMRI), Qingdao 266101
    3. State Key Laboratory for Corrosion and Protection, Shenyang 110016

Received date: 2010-12-29

  Revised date: 2011-03-24

  Online published: 2011-06-11

Abstract

In this paper, the effect of hydrostatic pressure on the corrosion behaviors of two steels was investigated by weight loss test, electrochemical measurements, rust layer analysis and morphology observation in natural seawater environment with high–pressure in lab. The results showed that X steel was inclined to being corroded. With the increase of hydrostatic pressure, the corrosion resistance of two steels were deteriorated, which were attributable to the increase of the anodic reaction rate. Hydrostatic pressure had little effect on oxygen diffusion reductin process of X steel. Howeve, the cathodic current density of Y steel under higher hydrostatic pressure decreased because the coosion products were directly involved in cathodic reduction reaction. And with the increase of hydrostatic pressure, the morphology of two steels changed significantly and dfferently. Under high pressure, some shallo–dish shape localized corrosion appeared on the surface of X steel whereas on the surface of Y steel some tunnel localized crrsion appeared.

Cite this article

LIU Jie , LI Xiang-Bei , YU Jia . EFFECT OF HYDROSTATIC PRESSURE ON THE CORROSION BEHAVIORS OF TWO LOW ALLOY STEELS[J]. Acta Metall Sin, 2011 , 47(6) : 697 -705 . DOI: 10.3724/SP.J.1037.2010.00705

References

[1] Wang J, Meng J, Tang X, Zhang W. J Chin Soc Corros Prot, 2007; 27: 1

(王佳, 孟洁, 唐晓, 张伟. 中国腐蚀与防护学报, 2007; 27: 1)

[2] Guo W M, Li W J. Equip Enviro Eng, 2006; 3: 60

(郭为民, 李文军. 装备环境工程, 2006; 3: 60)

[3] Xu L K, Li W J, Chen G Z. Mari Sci, 2005; 29: 1

(许立坤, 李文军, 陈光章. 海洋科学, 2005; 29: 1)

[4] Guo W M, Li W J, Chen G Z. Equip Enviro Eng, 2006; 3: 10

(郭为民, 李文军, 陈光章. 装备环境工程, 2006; 3: 10)

[5] Schumacher M. Seawater Corrosion Handbook, New Jersey: Noyes Data Corporation, 1979: 107

[6] Dexter S. Corrosion, 1980; 36: 423

[7] Sawant S, Wagh A. Corros Prevent Contr, 1990; 37: 154

[8] Venkatesan R, Venkatasamy M, Bhaskaran T, Dwarakadasa E. Br Corros, 2002; 37: 257

[9] Chen S, Hartt W, Wolfson S. Corrosion, 2003; 59: 721

[10] Beccaria A M, Poggi G, Castello G. Br Corros, 1986;21: 19

[11] Beccaria A M, Poggi G, Gingaud D, Castello P. Br Corros,1994; 29: 65

[12] Beccaria A M, Poggi G, Arfelli M, Mattongno D. Corros Sci, 1993; 34: 989

[13] Chen S, Hartt W. Corrosion, 2002; 58: 38

[14] Beccaria A M, Poggi G, Gingaud D, Castello G. Br Corros, 1995; 30: 283

[15] Liu B, Cong Y, Zhang T, Shao Y W, Meng G Z,Wang F H. Corros Sci Prot Technol, 2009; 21: 5

(刘斌, 丛园, 张涛, 邵亚薇, 孟国哲, 王福会. 腐蚀科学与防护技术, 2009; 21: 5)

[16] Zhang T, Yang Y G, Shao Y W. Electrochim Acta, 2009; 15: 3915

[17] Yang Y G, Zhang T, Shao Y W, Meng G Z, Wang F H. Corros Sci, 2010; 52: 2697

[18] Practice for Laboratory Immersion Corrosion Testing of Metals, ASTM Standard G31, 1999

[19] Raman A, Kuban B, Razvan A. Corros Sci, 1991; 31: 1295

[20] Dunnwald J, Otto A. Corros Sci, 1989; 29: 1167

[21] Hu T, Lu X, Yan Y, Fu Y Y, Zhang H, Zhang S L. Spectrosc Spectr Anal, 2004; 24: 1072

(胡涛, 路欣, 阎研, 傅云义, 张 酣, 张树霖. 光谱学与光谱分析, 2004; 24: 1072)

[22] Xiao H, Wang S, Huang Z Z, Lin D Y. J Univ Sci Technol Beijing, 1997; 9: 476

(肖珩, 汪崧, 黄震中, 林定一. 北京科技大学学报, 1997; 9: 476)

[23] Li Y T, Li T X, Hou B R, Zhang J L. Oceanol Limnol Sin, 1998; 29: 651

(李言涛, 李延旭, 侯保荣, 张经磊. 海洋与湖沼, 1998; 29: 651)

[24] Antony H, Perrin S, Dillmann Ph, Legrand L, Chauss´e A. Electrochim Acta, 2007; 52: 7754

[25] Stratmann M, M¨uller J. Corros Sci, 1994; 36: 327

[26] Stratmann M, Hoffmann K. Corros Sci, 1989; 29: 1329

[27] Stratmann M, Streckel H. Corros Sci, 1990; 30: 697
Outlines

/

〈 〉