Based on the thermal–mechanical coupling finite element model described in Part I of present work, the thermal behavior of one high strength ship plate steel solidifying in slab continuous casting mold was simulated with the practical continuous casting conditions of a steel plant, and the availability of the model was verified by in–plant measurement temperature. With this model, the thickness distributions and thermal behavior of air gap, mold flux (including liquid flux and solidified flux), and the variation characteristics of heat flux and surface temperature, as well as the influence of casting speed, mold taper, and mold flux properties on thermal behavior of the steel solidifying in mold were investigated.
SA Zhao-Tian
,
ZHU Miao-Yong
. SIMULATION OF THERMAL BEHAVIOR DURING STEEL SOLIDIFICATION IN SLAB CONTINUOUS CASTING MOLD II. Model Verification and Results Analysis[J]. Acta Metall Sin, 2011
, 47(6)
: 678
-687
.
DOI: 10.3724/SP.J.1037.2010.00664
[1] Yamauchi A, Emi T, Seetharaman S. ISIJ Int, 2002; 42: 1084
[2] Cho J W, Shibata H, Emi T. ISIJ Int, 1998; 38: 440
[3] Yamauchi A, Sorimachi K, Sakuraya T, Fujii T. ISIJ Int, 1993; 33: 140
[4] Thomas B G, Moitra A, McDavid R. Iron Steelmaker (ISS Transaction), 1996; 23: 57
[5] CaZ Z, Zhu M Y. Acta Metall Sin, 2011; 47: 671
(蔡兆镇, 朱苗勇. 金属学报, 2011; 47: 671)
[6] Liu X D, Zhu M Y, Cheng N L. Acta Metall Sin, 2006; 42:1081
(刘旭东, 朱苗勇, 程乃良. 金属学报, 2006; 42: 1081)
[7] Li C S, Thomas B G. Metall Trans, 2004; 35B: 1151
[8] Han H N, Lee J E, Yeo T, Won Y M, Kim K H, Oh K H, Yoon J K. ISIJ Int, 1999; 39: 445
[9] Mizukami H, Murakami K. Tetsu Hagan´e, 1977; 63: S652
(水上秀昭, 村上腾彦. 铁と钢,1977; 63: S652)
[10] Uehara M, Samarasekera I V, Brimacombe J K. Ironmaking Steelmaking, 1986; 13: 138
[11] Anand L. Trans ASME, 1982; 104: 12
[12] Brown S B, Kim K H, Anand L. Int J Plast, 1989; 5: 95
[13] Koric S, Thomas B G. J Mater Process Technol, 2008; 197:408
[14] Saraswat R, Maijer D M, Lee P D, Mills K. ISIJ Int, 2007;47: 95
[15] Nakada H, Susa M, Seko Y, Hayashi M, Nagata K. ISIJ Int, 2008; 48: 446