论文

INFLUENCES OF Fe3C AND PEARLITE ON THE ELECTROCHEMICAL CORROSION BEHAVIORS OF LOW CARBON FERRITE STEEL

  • YU Li-Wei ,
  • DU Cui-Wei ,
  • LIU Zhi-Yong ,
  • ZENG Xiao-Xiao ,
  • LI Xiao-Gang
Expand
  • Key Laboratory of Corrosion and Protection, Ministry of Education of China, Corrosion and Protection Center, University
    of Science and Technology Beijing, Beijing 100083

Received date: 2011-04-06

  Revised date: 2011-05-13

  Online published: 2011-10-11

Supported by

Supported by National Natural Science Foundation of China (Nos.50971016 and 50901041) and Fundamental Research Funds for the Central Universities (No.FRF–TP–09–029B)

Abstract

The microstructure of X80 pipeline steel welding joint, consisted of Fe3C and degenerated pearlite, was simulated by carburizing treatment. The effects of Fe3C and pearlite on the electrochemical properties of bainitic ferrite steel and localized corrosion occurrence regularity in Yingtan soil simulation solution were investigated by scanning Kelvin probe (SKP), scanning vibrating probe (SVP) and local electrochemical impedance spectroscopy (LEIS), combined with immersion test. It is demonstrated that the corrosion potential of degenerated pearlite is lower than bainitic ferrite, and decreases with increasing Fe3C content. Localized corrosion occurs on the surface of the carburized sample in Yingtan soil simulation solution. The anodic oxidation process is observed to be initiated on the carburized degenerated pearlite, whereas the cathodic reaction involving dissolved H+ is on bainitic ferrite, and the anodic current density increases with increasing Fe3C concentration. As the ion contents of the soil simulation solution doubled, the anodic dissolution of degenerated pearlite increases, and the local impedance of the electrode decreases.

Cite this article

YU Li-Wei , DU Cui-Wei , LIU Zhi-Yong , ZENG Xiao-Xiao , LI Xiao-Gang . INFLUENCES OF Fe3C AND PEARLITE ON THE ELECTROCHEMICAL CORROSION BEHAVIORS OF LOW CARBON FERRITE STEEL[J]. Acta Metall Sin, 2011 , 47(10) : 1227 -1232 . DOI: 10.3724/SP.J.1037.2011.00198

References

[1] Carneiro R A, Ratnapuli R C, de Freitas Cunha Lins V. Mater Sci Eng, 2003; A357: 104

[2] Gonzalez–Rodriguez J G, Casales M, Salinas–Bravo V M. Corrosion, 2002; 58: 584

[3] Chu R, Chen W, Wang S H. Corrosion, 2004; 60: 275

[4] Bulger J T, Lu BT, Luo J L. J Mater Sci, 2006; 41: 5001

[5] Albarran J L, Martinez L, Lopez H F. Corros Sci, 1999; 41: 1037

[6] Lee S, Kim B, Kwon D. Metall Mater Trans, 1992; 23A: 2803

[7] Liu Z Y, Li X G, Du C W. Corros Sci, 2009; 51: 895

[8] Kobayashi Y, Ume K, Hyodo T. Corros Sci, 1987; 27: 1117

[9] Fan Z, Liu J Y, Li S L, Zhang T J. J Southwest Petro Univ (Sci Technol Ed), 2009; 31: 171

(范舟, 刘建仪, 李士伦, 张天江. 西南石油大学学报(自然科学版), 2009; 31: 171)

[10] Santos T F A, Hermenegildo T F C, Afonso C R M. Eng Fract Mech, 2010; 77: 2937

[11] Ale R M, Rebello J M A, Charlier J. Mater Charact, 1996; 37: 89

[12] Xue X H, Zhou Y, Qian B N, Li J L, Lou S N. J Shanghai Jiaotong Univ, 2003; 37: 1854

(薛小怀, 周 昀, 钱百年, 李晶丽, 楼松年. 上海交通大学学报, 2003; 37: 1854)

[13] Souto R M, Gonzalez–Garcia Y, Bastos A C. Corros Sci, 2007; 49: 4568

[14] Simôes A M, Bastos A C, Souto R M. Corros Sci, 2007; 49: 726

[15] Krawiec H, Vignal V, Oltra R. Electrochem Commun, 2004; 6: 655

[16] Annergren I, Zou F, Thierry D. Electrochim Acta, 1999; 44: 4383

[17] Tang X, Cheng Y F. Appl Surf Sci, 2008; 254: 5199

[18] Zou F, Dominigue T, Han W A. Corros Sci Protect Technol, 1997; 9: 276

(邹锋, Dominigue T, 韩文安. 腐蚀科学与防护技术, 1997; 9: 276)

[19] Zhang G A, Cheng Y F. Corros Sci, 2009; 51: 1714

[20] ASM Committee on Gas Carburizing. Carburizing and Carbonitriding. Ohio: American Society for Metals, 1977: 179

[21] Liu Z Y, Li X G, Du C W. Corros Sci, 2009; 51: 2863

[22] Ohnori Y. Trans ISIJ, 1972; 12: 128

[23] Stratmann M. Corros Sci, 1987; 27: 869

[24] Stratmann M, Streckel H, Bunsen B. Phys Chem, 1988, 92: 1244

[25] Park C J, Kwon H S. Corros Sci, 2002; 44: 2817

[26] Lo I H, Fu Y, Lin C J. Corros Sci, 2006; 48: 696

[27] Liu Z Y, Li X G, Du C W. Corros Sci, 2009; 51: 895

[28] Liu X, Mao X. Scr Mater, 1995; 33: 145

[29] Clover D, Kinsella B, Pejcic B. J Appl Electrochem, 2005; 35: 139

[30] Liu Z Y, Zhai G L, Du C W, Li X G. Acta Metall Sin, 2008; 44: 209

(刘智勇, 翟国丽, 杜翠薇, 李晓刚. 金属学报, 2008; 44: 209)
Outlines

/