论文

NUMERICAL SIMULATION OF HYDROGEN INDUCED DELAYED FRACTURE OF AISI4135 HIGH STRENGTH STEEL USING COHESIVE ZONE MODELING

  • YU Yan-Fei ,
  • GONG Jian-Ming ,
  • JIANG Wen-Chun ,
  • JIANG Yong ,
  • TANG Jian-Qun
Expand
  • 1) College of Mechanical and Power Engineering, Nanjing University of Technology, Nanjing 210009
    2) College of Mechanical and Electronic Engineering, China University of Petroleum, Dongying 257061

Received date: 2010-12-30

  Revised date: 2011-02-08

  Online published: 2011-05-11

Supported by

Supported by Foundation for Six Talents Peak of Jiangsu Province (No.06-D-035)

Abstract

High strength steels are susceptible to hydrogen induced delayed fracture (HIDF). A sequential coupling calculation on HIDF of high strength steel was developed based on cohesive zone modeling (CZM) using finite element program-ABAQUS. The calculation procedure contained three steps: elastic plastic stress analysis, stress assisted transient hydrogen diffusion and cohesive stress analysis using hydrogen dependent linear traction-separation law. Using this method, the prediction of fracture time and crack initiation location of pre-charged notched bar of AISI4135 high strength steel was obtained. The effects of stress concentration factor, initial hydrogen content, and tension load were also considered. The results show: (i) predictions of the time to fracture were in good quantitative agreement with the experimental results; the hydrogen dependent cohesive zone modeling can be used in prediction of failure in actual structures; (ii) crack initiation occurs when a critical hydrogen concentration at the location of stress peak is reached by accumulation, the critical hydrogen concentration is dependent on stress concentration factor and tension load, but independent of initial hydrogen content; (iii) as one of the three parameters mentioned above decreasing, the fracture initiation time and the critical hydrogen\linebreak concentration increase.

Cite this article

YU Yan-Fei , GONG Jian-Ming , JIANG Wen-Chun , JIANG Yong , TANG Jian-Qun . NUMERICAL SIMULATION OF HYDROGEN INDUCED DELAYED FRACTURE OF AISI4135 HIGH STRENGTH STEEL USING COHESIVE ZONE MODELING[J]. Acta Metall Sin, 2011 , 47(5) : 594 -600 . DOI: 10.3724/SP.J.1037.2010.00711

References

[1] Chu W Y, Qiao L J, Chen Q Z, Gao K W. Fracture and Environment Fracture. Beijing: Science Press, 2000: 126

(褚武扬, 乔利杰, 陈奇志, 高克玮. 断裂与环境断裂. 北京: 科学出版社, 2000: 126)

[2] Serebrinsky S, Carter E A, Ortiz M. J Mech Phys Solids, 2004; 52: 2403

[3] Liang Y, Sofronis P. J Mech Phys Solids, 2003; 51: 1509

[4] Olden V, Thaulow C, Johnsen R, Φstby E, Berstad T. Eng Fract Mech, 2008; 75: 2333

[5] Olden V, Thaulow C, Johnsen R, Φstby E. Scr Mater, 2007; 57: 615

[6] Scheider I, Pfuff M, Dietzel W. Eng Fract Mech, 2008; 75: 4283

[7] Wang M Q, Akiyama E, Tsuzaki K. Corros Sci, 2006; 48: 2189

[8] Dugdale D S. J Mech Phys Solids, 1960; 8: 100

[9] Barrenblatt G I. Adv Appl Mech, 1962; 7: 55

[10] Hillerborg A, Modeer M, Petersson P. Cement Concrete Res, 1976; 6: 773

[11] Needleman A. J Appl Mech, 1987; 54: 525

[12] Nguyen O, Ortiz M. J Mech Phys Solids, 2002; 50: 1727

[13] Jiang D E, Carter E A. Acta Mater, 2004; 52:4801

[14] Hondros E D, Seah M P. Metall Trans, 1977; 8A: 1363

[15] Van der Ven A, Ceder G. Phys Rev, 2003; 67B: 060101

[16] Tvergaard V, Hutchinson J W. J Mech Phys Solids, 1992; 40: 1377

[17] Wang M Q, Akiyama E, Tsuzaki K. Mater Sci Eng, 2005; A398: 37

[18] GerberichWW, Livne T, Chen X F, Kaczorowski M. Metall Trans, 1988; 19A: 1319

[19] Williams D P, Nelson H G. Metall Trans, 1970; 1: 63
Outlines

/

〈 〉