EFFECTS OF Bi ADDITION ON SOLIDIFICATION BEHAVIOR AND MICROSTRUCTURE OF AZ80 MAGNESIUM ALLOY

  • YU Ya-Xiao ,
  • FU Jun-Wei ,
  • YU Jing ,
  • LUO Tian-Jiao ,
  • DONG Xu-Guang ,
  • YANG Yuan-Sheng
Expand
  • Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016

Received date: 2010-11-10

  Revised date: 2010-12-24

  Online published: 2011-04-11

Supported by

Supported by National Basic Research Program of China (No.2007CB613705)

Abstract

The solidification behavior and as--cast microstructure in AZ80-Bi magnesium alloy were analysed by OM, SEM, XRD and DSC. Meanwhile, the evolution of the solidification microstructure of AZ80-2%Bi alloy was studied by heating-quenching experiments. The results show that the as-cast microstructure of AZ80-2%Bi consists of primary α-Mg matrix, divorced eutectic β-Mg17Al12 phase and Mg3Bi2 phase. The Mg3Bi2 phase exists in the flake-like and granule-like morphologies. With 2.0%Bi addition, the solidification procedure of AZ80 magnesium alloy is changed. The ternary eutectic transformation L→α-Mg+β-Mg17Al12+Mg3Bi2 (at 435 ℃) takes place during solidification of AZ80-2%Bi alloy instead of the binary eutectic transformation L→α-Mg+β-Mg17Al12 (at 437 ℃) in AZ80 alloy. Comparing with AZ80 alloy, the nucleating temperature of primary $\alpha$--Mg in AZ80--2\%Bi alloy is decreased from 568.8 ℃ to 562.6 ℃, and the eutectic temperature is also decreased from\linebreak 424.2 ℃ to 421.1 ℃.

Cite this article

YU Ya-Xiao , FU Jun-Wei , YU Jing , LUO Tian-Jiao , DONG Xu-Guang , YANG Yuan-Sheng . EFFECTS OF Bi ADDITION ON SOLIDIFICATION BEHAVIOR AND MICROSTRUCTURE OF AZ80 MAGNESIUM ALLOY[J]. Acta Metall Sin, 2011 , 47(4) : 410 -416 . DOI: 10.3724/SP.J.1037.2010.00604

References

[1] Avedesian M M, Baker H. Magnesium and Magnesium Alloys. Materials Park, OH: ASM International, 1999: 22

[2] Yang Z, Li J P, Zhang J X, Lorimer GW, Robson J. Acta Metall Sin (Engl Lett), 2008; 21: 313

[3] Mordike B L, Ebert T. Mater Sci Eng, 2001; A302: 37

[4] Tang W, Han E H, Xu Y B, Liu L. Trans Nonferrous Met Soc China, 2006; 16: 1725

[5] Yakubtsov I A, Diak B J, Sager C A, Bhattacharya B, MacDonald W D, Niewczas M. Mater Sci Eng, 2008; 496: 247

[6] Zhou J X, Wang B, Tong W H, Yang Y S. Acta Metall Sin, 2007; 43: 1171

(周吉学, 汪彬, 童文辉, 杨院生. 金属学报, 2007; 43: 1171)

[7] Yang M B, Pan F S, Cheng R J, Tang A T. Mater Sci Eng, 2008; A491: 440

[8] Hirai K, Somekawa H, Takigawa Y, Higashi K. Mater Sci Eng, 2005; A403: 276

[9] Min X G, Zhu M, Sun Y S, Xue F. Mater Sci Technol, 2002; 10: 93

(闵学刚, 朱旻, 孙扬善, 薛烽. 材料科学与工艺, 2002; 10: 93)

[10] Zhao Z D, Chen Q, Wang Y B, Shu D Y. Mater Sci Eng, 2009; A515: 152

[11] Xie J C, Li Q A, Wang X Q, Li J H. Trans Nonferrous Met Soc China, 2008; 18: 303

[12] Yuan G Y, Zhang W M, Sun Y S. J Southeast Univ, 1999; 29: 115

(袁广银, 张为民, 孙扬善. 东南大学学报, 1999; 29: 115)

[13] Yuan G Y, Sun Y S, Zhang W M. Foundry, 1998; (5): 5

(袁广银, 孙扬善, 张为民. 铸造, 1998; (5): 5)

[14] Yuan G Y, Sun Y S, Ding W J. Mater Sci Eng, 2001; A308: 38–44

[15] Ren W L, Li Q A, Shi Y J, Zhang X Y. Rare Met Cem Carbides, 2010; 38(3): 34

(任文亮, 李全安, 石雅静, 张兴渊. 稀有金属与硬质合金, 2010; 38(3): 34)

[16] Guo E J, Ma B X, Wang L P. J Mater Process Technol, 2008; 206: 161

[17] Zhang G Y, Zhang H, Fang G L, Li Y C. Acta Phys Sin, 2005; 54: 5288

(张国英, 张辉, 方戈亮, 李昱材. 物理学报, 2005; 54: 5288)

[18] Liu Z, Zhang K, Zeng X Q. Theoretical Basis and Application of Mg–based Lightweight Alloys. Beijing: Machine Industry Press, 2006: 61

(刘 正, 张奎, 曾小勤. 镁基轻质合金理论基础及其应用. 北京: 机械工业出版社, 2006: 61)

[19] Massalski T B, Okamoto H, Subramanian P R, Kacprzak L. Binary Alloy Phase Diagrams. Materials Park, OH: ASM International, 1990: 759

[20] Massalski T B, Okamoto H, Subramanian P R, Kacprzak L. Binary Alloy Phase Diagrams. Materials Park, OH: ASM International, 1990: 169

[21] Willars P, Prince A, Okamoto H. Ternary Alloy Phase Diagrams. Materials Park, OH: ASM International, 1995: 2845

[22] Wang C L. Phase Diagrams and Its Application. Beijing: Higher Education Press, 2008: 184

(王崇琳. 相图理论及其应用. 北京: 高等教育出版社, 2008: 184)

[23] Han Q, Eenik E A, Agnew S R, Viswanathan S. in Hryn J, ed., Magnesium Technology, Warrendale, PA: TMS, 2001: 81

[24] Gebelin J C, Suery M, Favier D. Mater Sci Eng, 1999; A272: 133
Outlines

/

〈 〉