Abstract

Addition of minor Sc and Zr to the Al–Mg alloys can effectively improve the recrystallization temperature and strength of the alloys due to the formation of L12 structured Al3(Sc, Zr) precipitates. To optimize the mechanical properties of the Al–Mg–Sc–Zr alloys, it is important to understand the precipitation behavior of the Al3(Sc, Zr) precipitates and the corresponding strengthening effect during the annealing of Al–Mg–Sc–Zr alloys. In this work, isothermal annealing at the temperatures between 250 and 450 ℃ was conducted to study the precipitation behavior of Al3(Sc, Zr) particles in the as–cast Al–6Mg–0.2Sc–0.15Zr alloy (mass fraction, %). The results show that dramatic precipitation hardening occurred with the formation of the coherent Al3(Sc, Zr) precipitates during the annealing. Precipitation rocess of the Al3(Sc, Zr) accelerates with the increase of the annealing temperature. After the sample was annealed at 300 ℃ for 24 h, the Al3(Sc, Zr) particles were in a size of 5 nm ad the yield strength of the as–cast alloy can be increased by 90 MPa. Severe coarsening of Al3(Sc, Zr) occurred when the annealing temperature is bove 400 ℃. After annealed at 450 ℃ for 24 h, average particle size of Al3(Sc, Zr) particles was found increase to 30 nm, wth the corresponding precipitation strengthening effect to be about 30 MPa.

Cite this article

DU Gang , YANG Wen , YAN De-Qing , RONG Li-Jian . HARDENING BEHAVIOR OF THE AS–CAST Al–Mg–Sc–Zr ALLOY[J]. Acta Metall Sin, 2011 , 47(3) : 311 -316 . DOI: 10.3724/SP.J.1037.2010.00645

References

[1] Filatov Y A, Yelagin V I, Zakharov V V. Mater Sci Eng, 2000; A280: 97

[2] Zhao W T, Yan D S, Rong L J. Acta Metall Sin, 2005; 41: 1150

(赵卫涛, 闫德胜, 戎利建. 金属学报, 2005; 41: 1150)

[3] Dougherty L M, Robertson I M, Vetrano J S. Acta  Mater, 2003; 51: 4367

[4] Seidman D N, Marquis E A, Dunand D C. Acta Mater, 2002; 50: 4021

[5] Davydov V G, Rostova T D, Zakharov V V, Filatov Y A, Yelagin V I. Mater Sci Eng, 2000; A280: 30

[6] Du G, Deng J W, Yan D S, Zhao M J, Rong L J. J Mater Sci Technol, 2009; 25: 749

[7] Nie B, Yin Z M, Zhu D P, Jiang F, He Z B. Chin J Rare Met, 2006; 30: 213

(聂波, 尹志民, 朱大鹏, 姜峰, 何振波. 稀有金属, 2006; 30: 213)

[8] Norman A F, Prangnell P B, Mcewen R S. Acta Mater, 1998; 46: 5715

[9] Iwamura S, Miura Y. Acta Mater, 2004; 52: 591

[10] Tian R Z, Wang Z T. Handbook of Aluminum Alloys. 2nd Ed., Changsha: Central South University Press, 2000: 64

(田荣璋, 王祝堂. 铝合金及其加工手册. 第二版, 长沙: 中南大学出版社, 2000: 64)

[11] Du G, Yang W, Yan D S, Rong L J. Chin J Nonferrous Met, 2010; 6: 1083

(杜刚, 杨文, 闫德胜, 戎利建. 中国有色金属学报, 2010; 6: 1083)

[12] Forbord B, Lefebvre W, Danoix F, Hallem H, Marthinsen K. Scr Mater, 2004; 51: 333

[13] Royset, J, Ryum, N. Mater Sci Eng, 2005; A396: 409

[14] Royset J, Hovland H, Ryum N. Mater Sci Forum, 2002; 396–402: 619

[15] Du G, Yan D S, Rong L J. Acta Metall Sin, 2008; 44: 1209

(杜刚, 闫德胜, 戎利建. 金属学报, 2008; 44: 1209)

[16] Huang Q Y, Li H K. Superalloy. Beijing: Metallurgical Industry Press, 2000: 22

(黄乾尧, 李汉康. 高温合金. 北京: 冶金工业出版社, 2000: 22)

[17] Fujikawa S I, Sugaya M, Takei H, Hirano K. J Less–Common Met, 1979; 63: 87

[18] Jo H H, Fujikawa S I. Mater Sci Eng, 1993; A171: 151
Outlines

/

〈 〉