STATE OF Fe-C ALLOY IN THE ELECTROMAGNETIC STEEL-TEEMING SYSTEM

  • GAO Ao ,
  • YU Jiang ,
  • LI De-Jun ,
  • CI Hai-Shan ,
  • DIAO Li-Jia ,
  • SHI Ji-Cheng
Expand
  • Key Laboratory of Electromagnetic Processing of Materials, Ministry of Education, Northeastern University, Shenyang 110819

Received date: 2010-08-20

  Revised date: 2010-11-03

  Online published: 2011-02-11

Supported by

Supported by Science and Technology Program of Liaoning Province (No.2008221015), Liaoning Bai Qian Wan Talents Program and Program of Introducing Talents of Discipline to University (No.B07015)

Abstract

A new method (electromagnetic steel-teeming method) using electromagnetic induction heating in slide-gate was proposed to overcome the disadvantage of the pollution of the traditional nozzle sand on the molten steel. The basic idea of this new process is to melt part or whole of the new ladle well-packing material (i.e. Fe-C alloy with similar composition of the molten steel), which becomes the substitute of the traditional nozzle sand, and achieve smoothly molten steel-teeming. In the experiment, the state of the Fe-C alloy well-packed in the upper nozzle was examined when the ladle held molten steel using the self-designed electromagnetic steel-teeming simulation facility. The results showed that the F-C alloy in the upper nozzle were divided into liquid Fe-C alloy, solidified Fe-C alloy, liquid-sintered, solid-sintered and original layers. The solidified, liquid-sintered and solid-sintered layers could prevent the molten steel flow into the upper nozzle from destroing the slide plate. The blocking layers could be melted with induction heating to achieve electromagnetic steel-teeming. In addition, the position of the liquid/solid interface of the Fe-C alloy in the upper nozzle was investigated. The length of liquid Fe-C alloy increased with the increase of time after molten steel poured into the ladle and then kept in a certain length. Furthermore, the position of the interface increased with the increase of melting points which were related to the composition of the Fe-C alloy. The experimental results indicated that 100% automatically teeming of the ladle would be achieved after using the electromagnetic steel-teeming technology.

Cite this article

GAO Ao , YU Jiang , LI De-Jun , CI Hai-Shan , DIAO Li-Jia , SHI Ji-Cheng . STATE OF Fe-C ALLOY IN THE ELECTROMAGNETIC STEEL-TEEMING SYSTEM[J]. Acta Metall Sin, 2011 , 47(2) : 219 -223 . DOI: 10.3724/SP.J.1037.2010.00418

References

[1] Zhang L F, Rietow B, Thomas B G, Eakin K. ISIJ Int, 2006; 46: 670

[2] Mazzaferro G M, Piva M, Ferro S P, Bissio P, Iglesias M, Calvo A, Goldschmit M B. Ironmaking Steelmaking, 2004; 31: 503

[3] Tanaka H, Nishihara R, Miura R, Tsujino R, Kimura T, Nishi T, Imoto T. ISIJ Int, 1994; 34: 868

[4] Tanaka H, Nishihara R, Kitagawa I, Tsujino R. ISIJ Int, 1993; 33: 1238

[5] Pan H C, Ko Y C. Ironmaking Steelmaking, 1992; 19: 390

[6] Adamo P, Arienzo M, Bianco M R, Terribile F, Violante P. Sci Total Envir, 2002; 295: 17

[7] Ndiokwere C L, Ezihe C A. Environ Int, 1990; 16: 291

[8] Ma G J, Garbers–Craig A M. J Hazard Mater, 2009; 169: 210

[9] Gonzalez–Miqueo L, Elustondo D, Lasheras E, Santamaria J M. Chemosphere, 2010; 78: 965

[10] He J C, Marukawa K, Wang Q. Chin Pat, ZL1810417, 2006

(赫冀成, 丸川雄净, 王强. 中国专利, ZL1810417, 2006)

[11] Gao A, Wang Q, He J C. J Northeast Univ (Nat Sci), 2010; 31: 515

(高翱, 王强, 赫冀成. 东北大学学报(自然科学版), 2010; 31: 515)

[12] Gao A, Wang Q, Li D J, Jin B G, Wang K, He J C. Acta Metall Sin, 2010; 46: 634

(高 翱, 王 强, 李德军, 金百刚, 王凯, 赫冀成. 金属学报, 2010; 46: 634)

[13] Gao A, Wang Q, Li D J, Jin B G, Wang K, He J C. ISIJ Int, 2010; 50: 1770

[14] Tian H X, Mao Z Z, Wang A N. ISIJ Int, 2009; 49: 58

[15] Olika B, Bjorkman B. Scand J Metall, 1993; 22: 213

[16] Ganguly S, Chakraborty S. ISIJ Int, 2004; 44: 537

[17] Nemchinov A I, Pevzner M B. Metallurgist, 1985; 29: 236

[18] Subramanian R Schneibel J H. Mater Sci Eng, 1998; A244: 103

[19] Plucknett K P, Becher P F, Subramanian R. J Mater Res, 1997; 12: 2515

[20] Muscat D, Shanker K, Drew R A L. Mater Sci Technol, 1992; 8: 971

[21] Chen J X. Handbook of Continuous Casting. Beijing: Metallurgial Industry Press, 1991: 80

(陈家祥. 连续铸钢手册. 北京: 冶金工业出版社, 1991: 80)
Outlines

/

〈 〉