论文

Al-Cr COATINGS PREPARED BY DIFFUSION AT LOW TEMPERATURE AND ITS PHASE CHARACTERIZATION

  • LI Wen-Chuan ,
  • SA Jun ,
  • LING Guo-Beng
Expand
  • Department of Materials Science and Engineering, Zhejiang University, Hangzhou 310027

Received date: 2010-07-08

  Revised date: 2010-10-21

  Online published: 2011-02-11

Abstract

The Al-Cr coating exhibits a good steam oxidation resistance and can act as tritium permeation barrier. It is necessary to prepare Al-Cr coating at low temperatures to avoid detrimental effect on the mechanical properties of the substrate. In the present study, a new process was proposed to prepare Al-Cr coating by electrodeposition of Cr/Al composite coatings firstly, and then heat treatment at low temperatures. The Cr/Al composite coatings were obtained by electrodepositing Cr from aqueous solution followed by electrodepositing Al from AlCl3-EMIC ionic liquid. Effects of the temperature of heat treatment on the composition and phase of alloy layers were studied by using OM, SEM, BSE, EDS and XRD. The results showed that an Al-Cr alloy layer at the Cr/Al interface was formed even at low temperature of 540 ℃ by the interdiffuse between Al and Cr coating. The different Al-Cr alloy layers could be formed by controlling the thickness of Cr and Al in Cr/Al composite coatings. For 6.5 μm Cr/15 μm Al composite coating, the main phase was Al8Cr5 for 960 min heat treatment at 640 ℃, and for 1.6 μm Cr/15 μm Al composite coatings treated at 600 ℃ for 30 min, the main phase of alloy layer was Al4Cr.

Cite this article

LI Wen-Chuan , SA Jun , LING Guo-Beng . Al-Cr COATINGS PREPARED BY DIFFUSION AT LOW TEMPERATURE AND ITS PHASE CHARACTERIZATION[J]. Acta Metall Sin, 2011 , 47(2) : 231 -235 . DOI: 10.3724/SP.J.1037.2010.00331

References

[1] Zhang Y, Pint B A, Cooley K M, Haynes J A. Surf Coat Technol, 2008; 202: 3839

[2] Konys J, Aiello A, Benamati G, Giancarli L. Fus Sci Technol, 2005; 47: 844

[3] Han S L, Li H L, Wang S M, Jiang L J, Liu X P. Int J Hydrogen Energy, 2010; 35: 2689

[4] Geib F D, Rapp R A. Oxid Met, 1993; 40: 213

[5] Xiang Z D, Datta P K. Surf Coat Technol, 2004; 184: 108

[6] Wang Y Q, Zhang Y, Wilson D A. Surf Coat Technol, 2010; 204: 2737

[7] Si X, Lu B, Wang Z. J Mater Sci Technol, 2009; 25: 433

[8] Xiang Z D, Rose S R, Datta P K, Scheeffer M. Surf Coat Technol, 2009; 203: 1225

[9] Li Y, Ling G P, Liu K Z, Chen C A, Zhang G K. Trans Mater Heat Treat, 2009; 30(5): 182

(李岩, 凌国平, 刘柯钊, 陈长安, 张桂凯. 材料热处理学报, 2009; 30(5): 182)

[10] Nagasaki S, Hirabayashi M. Binary Alloy Phase Diagrams, Tokyo: AGNE Gijutsu Center Co. Ltd., 2002: 29

[11] He Z B, Zou B S, Kuo K H. J Alloys Compd, 2006; 417: L4

[12] Cao B B, Kuo K H. J Alloys Compd, 2008; 458: 238

[13] Wen K Y, Chen Y L, Kuo K H. Metall Trans, 1992; 23A: 2437

[14] Brushko B, Przei´orzy´nski B, Kowalska–Strzeciwilk E, Surowiec M. J Alloys Compd, 2006; 420: L1

[15] Barbier F, Manuelli D, Bouch´e K. Acta Metall, 1997; 36: 425

[16] Tunca N, Delamore G W, Smith R W. Metall Trans, 1990; 21A: 2919

[17] Mahdouk K, Gachon J C. J Phase Equilibria, 2000; 21(2): 157

[18] Okamoto H. J Phase Equilibria Diffus, 2008; 29(1): 112

[19] Grushko B, Kowalska–Strze.ciwilk E, Przepiorzynski B, Surowiec M. J Alloys Compd, 2005; 402: 98
Outlines

/