The effect of Cu content on the corrosion resistance of Zr-1%Nb-xCu (x=0.05%-0.5%, mass fraction) was investigated in superheated steam at 500 ℃ and 10.3 MPa by autoclave tests. The microstructures of the alloys and oxide films on the corroded specimens were observed by TEM and SEM, respectively. The results showed that when the Cu content was below 0.2%, the corrosion resistance of the alloys was markedly improved with the increase of Cu content, while further addition of Cu did not lead to a further improvement in the corrosion resistance. When the Cu content was below 0.2%, the Cu mainly dissolved in the α-Zr matrix. And when the Cu content was more than 0.2%, part of Cu precipitated as Zr2Cu second phase particles. When the α-Zr matrix was oxidized, the Cu dissolved in the α-Zr could delay the process that the vacancies in the oxide film diffused and coalesced to form pores, and the pores developed into micro-cracks. Therefore, the corrosion resistance of the alloys was enhanced. It can be concluded that the Cu concentration in the α-Zr matrix, rather than the second phase particles containing Cu, is the main reason that the addition of Cu improves the corrosion resistance of M5 alloy in superheated steam at 500 ℃ and 10.3 MPa.
LI Shi-Lu
,
YAO Mei-Yi
,
ZHANG Xin
,
GENG Jian-Qiao
,
PENG Jian-Tiao
,
ZHOU Bang-Xin
. EFFECT OF ADDING Cu ON THE CORROSION RESISTANCE OF M5 ALLOY IN SUPERHEATED STEAM AT 500℃[J]. Acta Metall Sin, 2011
, 47(2)
: 163
-168
.
DOI: 10.3724/SP.J.1037.2010.00352
[1] Park J Y, Choi B K, Yoo S J, Jeong Y H. J Nucl Mater, 2006; 359: 59
[2] Park J Y, Yoo S J, Choi B K, Jeong Y H. J Alloys Compd, 2007; 437: 274
[3] Hong H S, Moon J S, Kim S J, Lee K S. J Nucl Mater, 2001; 297: 113
[4] Jeong Y H, Kim H G, Kim T H. J Nucl Mater, 2003; 317: 1
[5] Kim J M, Jeong Y H. J Nucl Mater, 1999; 275: 74
[6] Charquet D, Hahn R, Ortlieb E, Gros J P, Wadier J F. In: Van Swam L F P, Eucken C M eds., Zirconium in the Nuclear Industry: 8th International Symposium, ASTM STP 1023, Baltimore: ASTM International, 1988: 405
[7] Anada H, Takeda K. In: Sabol G P, Bradley E R eds., Zirconium in the Nuclear Industry: 11th International Symposium, ASTM STP 1295, Ann Arbor: ASTM International, 1996: 35
[8] Wadman B, Lai Z, Andr´en H O, Nystr¨om A L, Rudling P, Pettersson H. In: Garde A M, Bradley E R eds., Zirconium in the Nuclear Industry: 10th International Symposium, ASTM STP 1245, Ann Arbor: ASTM International, 1994: 579
[9] Jeong Y H, Lee K O, Kim H G. J Nucl Mater, 2002; 302: 9
[10] Kim H G, Jeong Y H, Kim T H. J Nucl Mater, 2004; 326: 125
[11] Jeong Y H, Kim H G, Kim D J. J Nucl Mater, 2003; 323: 72
[12] Abe T, Shimono M, Ode M, Onodera H. Acta Mater, 2006; 54: 909
[13] Yang W D. Reactor Materials Science. 2nd Ed., Beijing: Atomic Energy Press, 2006: 260
(杨文斗. 反应堆材料学. 第二版. 北京: 原子能出版社, 2006: 260)
[14] Zhou B X, Li Q, Yao M Y, Liu W Q. Nucl Power Eng, 2005; 26: 364
(周邦新, 李 强, 姚美意, 刘文庆. 核动力工程, 2005; 26: 364)
[15] Zhou B X, Li Q, LiuWQ, YaoMY, Chu Y L. Rare Metal Mat Eng, 2006; 35: 1009
(周邦新, 李强, 刘文庆, 姚美意, 褚于良. 稀有金属材料与工程, 2006; 35: 1009)
[16] Zhou B X, Li Q, Yao M Y, Liu W Q, Chu Y L. J ASTM Intl, 2008; 5: 360