论文

MODELING AND SIMULATION ON MICROPOROSITY FORMED DURING SQUEEZE CASTING OF ALUMINUM ALLOY

  • HAN Zhi-Jiang ,
  • YANG Wen ,
  • LIU Bai-Cheng
Expand
  • 1) Key Laboratory for Advanced Materials Processing Technology (Ministry of Education), Department of Mechanical Engineering, Tsinghua University, Beijing 100084
    2) School of Mechanical and Automotive Engineering, South China University of Technology, Guangzhou 510640 
    3) State Key Laboratory of Automotive Safety and Energy, Department of Automotive Engineering, Tsinghua University,  Beijing 100084

Received date: 2010-06-30

  Revised date: 2010-10-26

  Online published: 2011-01-11

Supported by

Supported by National Natural Science Foundation of China (Nos.50675113 and 50875143)

Abstract

A mathematical model for simulating the microporosity in squeeze casting of aluminum alloy has been developed, in which the heat transfer, solidification shrinkage, feeding flow, pressure transfer, and hydrogen conservation were taken into account. The shrinkage induced flow and the pressure drop in the mushy zone were calculated by solving continuity and momentum equations. A mechanical model was solved for obtaining the pressure transferred into the central area of the casting. By coupling the pressure drop with the pressure transferred into the central area, the pressure distribution in the mushy zone was calculated. Based on the hydrogen conservation equation, the microporosity volume fraction was calculated by referring to the pressure value in the mushy zone. The squeeze casting processes of aluminum alloy under different process conditions were simulated and the simulation results were compared with experimental results. It was shown that the simulation results agree well with the experimental results, and the increases in applied pressure and mould temperature tend to reduce the microporosity in the castings.

Cite this article

HAN Zhi-Jiang , YANG Wen , LIU Bai-Cheng . MODELING AND SIMULATION ON MICROPOROSITY FORMED DURING SQUEEZE CASTING OF ALUMINUM ALLOY[J]. Acta Metall Sin, 2011 , 47(1) : 7 -16 . DOI: 10.3724/SP.J.1037.2010.00313

References

[1] Ghomashchi M R, Vikhrov A. J Mater Process Technol, 2000; 101: 1

[2] Qi P X. Spec Cast Nonferrous Alloys, 1998; 18(4): 32

(齐丕骧. 特种铸造及有色合金, 1998; 18(4): 32)

[3] Luo S J, Chen B G, Qi P X. Liquid Forging and Squeeze Casting Technology. Beijing: Chemical Industry Press, 2007: 1

(罗守靖, 陈炳光, 齐丕骧. 液态模锻与挤压铸造技术. 北京: 化学工业出版社, 2007: 1)

[4] Major J F. AFS Trans, 1998; 105: 901

[5] Samuel A M, Samuel F H. Metall Mater Trans, 1995; 26A: 2359

[6] Lee C D. Mater Sci Eng, 2007; A464: 249

[7] Lee P D, Chirazi A, See D. J Light Met, 2001; (1): 15

[8] Stefanescu D M. Int J Cast Met Res, 2005; 18(3): 129

[9] Gui Z L, Dai T, Zhu M F. Spec Cast Nonferrous Alloys, 2007; 27: 766

(桂仲林, 戴挺, 朱鸣芳. 特种铸造及有色合金, 2007; 27: 766)

[10] Kubo K, Pehlke R D. Metall Trans, 1985; 16B: 359

[11] Poirier D R, Yeum K, Maples A L. Metall Trans, 1987; 18A: 1979

[12] Shivkumar S, Apelian D, Zou J. AFS Trans, 1990; 98: 897

[13] Sabau A S, Viswanathan S. Metall Mater Trans, 2002; 33B: 243

[14] Pequet C H, Gremaud M, Rappaz M. Metall Mater Trans, 2002; 33A: 2095

[15] Zhao H D, Wu C Z, Li Y Y, Ohnaka I. Acta Metall Sin, 2008; 44: 1340

(赵海东, 吴朝忠, 李元元, 大中逸雄. 金属学报, 2008; 44: 1340)

[16] Atwood R C, Sridhar S, Zhang W, Lee P D. Acta Mater, 2000; 48: 405

[17] Lee P D, Chirazi A, Atwood R C, Wang W. Mater Sci Eng, 2004; A365: 57

[18] Wang J S, Lee P D. Int J Cast Met Res, 2007; 20(3): 151

[19] Backer G, Wang Q G. Metall Mater Trans, 2007; 38B: 533

[20] Carlson K D, Lin Z P, Beckermann C. Metall Mater Trans, 2007; 38B: 541

[21] Han Z Q, Zhu W, Liu B C. Acta Metall Sin, 2009; 45: 356

(韩志强, 朱维, 柳百成. 金属学报, 2009 45: 356)

[22] Zhu W, Han Z Q, Liu B C. Acta Metall Sin, 2009 45: 363

(朱维, 韩志强, 柳百成. 金属学报, 2009; 45: 363)

[23] Anyalebechi P N. Acta Metall, 1995; 33: 1209

[24] Lewis R W, Han Z Q, Gethin D T. C R Mec, 2007: 335: 287

[25] Yang W, Li J X, Han Z Q, Zhao H D, Liu B C. Spec Cast Nonferrous Alloys, 2010; 30: 54

(杨文, 李金玺, 韩志强, 赵海东, 柳百成. 特种铸造及有色合金, 2010; 30: 54)
Outlines

/

〈 〉