Abstract

Strengthening materials is a central objective of materials research. Traditional approaches to strengthen materials, including solid solution strengthening, second phase strengthening, grain refinement strengthening, dispersion strengthening and work hardening strengthening etc., aim at creation of internal defects and boundaries so as to obstruct the motion of dislocations. Such strategies for strengthening invariably compromise the ductility and electrical conductivity of the material. By reviewing recent advances in our understanding of nanostructured metals and alloys, we propose a novel approach to optimize the strength, ductility and the electrical conductivity of materials by means of coherent twin boundaries at nano-meter scale. We assess current understanding of strengthening mechanism of twin boundaries (instead of incoherent boundaries as conventionally used). Additionally, some mechanical properties (such as strength, ductility, strain rate sensitivity, work hardening) and the physical properties (electrical conductivity and electrical migration) as well as the relative preparation techniques of the metallic materials with nano-scale twins will be reviewed in this paper.

Cite this article

LV Lei , LV Ke . METALLIC MATERIALS WITH NANO--SCALE TWINS[J]. Acta Metall Sin, 2010 , 46(11) : 1422 -1427 . DOI: 10.3724/SP.J.1037.2010.00462

References

[1] Lu K, Lu L, Suresh S. Science, 2009; 324: 349 [2] Hall E O. Proc Phys Soc London, 1951; 64B: 747 [3] Petch N J. J Iron Steel Inst, 1953; 174: 25 [4] Meyers M A, Mishra A, Benson D J. Prog Mater Sci, 2006; 51: 427 [5] Wei Q, Cheng S, Ramesh K T, Ma E. Mater Sci Eng, 2004; A381: 71 [6] Chen J, Lu L, Lu K. Scr Mater, 2006; 54: 1913 [7] Koch C C, Morris D G, Lu K, Inoue A. MRS Bull, 1999; 24: 54 [8] Koch C C. Scr Mater, 2003; 49: 657 [9] Ma E. Scr Mater, 2003; 49: 663 [10] Christian J W, Mahajan S. Prog Mater Sci, 1995; 39: 1 [11] Meyers M A, Chawla K K. Mechanical Behavior of Materials. Upper Saddle River, New Jersey: Pretice Hall, 1999: 1 [12] Lu L, Shen Y F, Chen X H, Qian L H, Lu K. Science, 2004; 304: 422 [13] Shen Y F, Lu L, Lu Q H, Jin Z H, Lu K. Scr Mater, 2005; 52: 989 [14] Jin Z H, Gumbsch P, Albe K, Ma E, Lu K, Gleiter H, Hahn H. Acta Mater, 2008; 56: 1126 [15] Jin Z H, Gumbsch P, Ma E, Albe K, Lu K, Hahn H, Gleiter H. Scr Mater, 2006; 54: 1163 [16] Lu L, Schwaiger R, Shan Z W, Dao M, Lu K, Suresh S. Acta Mater, 2005; 3: 2169 [17] Zhang X, Wang H, Chen X H, Lu L, Lu K, Hoagland R G, Misra A. Appl Phys Lett, 2006; 88: 173116 [18] Lu L, Chen X, Huang X, Lu K. Science, 2009; 323: 607 [19] Li X,Wei Y, Lu L, Lu K, Gao H. Nature, 2010; 464: 877 [20] Shen Y F, Lu L, Dao M, Suresh S. Scr Mater, 2006; 55: 319 [21] Lu L, Dao M, Zhu T, Li J. Scr Mater, 2009; 60: 1062 [22] Lu L, Zhu T, Shen Y F, Dao M, Lu K, Suresh S. Acta Mater, 2009; 57: 5165 [23] Zhao W S, Tao N R, Guo J Y, Lu Q H, Lu K. Scr Mater, 2005; 53: 745 [24] Tao N R, Lu K. J Mater Sci Technol, 2007; 23: 771 [25] Zhang Y, Tao N R, Lu K. Acta Mater, 2008; 56: 2429 [26] Li Y S, Tao N R, Lu K. Acta Mater, 2008; 56: 230 [27] Qin E W, Lu L, Tao N R, Lu K. Scr Mater, 2009; 60: 539 [28] Qin E W, Lu L, Tao N R, Tan J, Lu K. Acta Mater, 2009; 57: 6215 [29] Ustinov A I, Skorodzievski V S, Fesiun E V. Acta Mater, 2008; 56: 3770 [30] Dao M, Lu L, Shen Y F, Suresh S. Acta Mater, 2006; 54: 5421 [31] Chen K C, Wu W W, Liao C N, Chen L J, Tu K N. Science, 2008; 321: 1066 [32] Zhang X, Misra A,Wang H, Shen T D, Nastasi M, Mitchell T E, Hirth J P, Hoagland R G, Embury J D. Acta Mater, 2004; 52: 995 [33] Zhang X, Misra A, Wang H, Lima A L, Hundley M F, Hoagland R G. J Appl Phys, 2005; 97: 094302 [34] Zhang X, Anderoglu O, Misra A, Wang H. Appl Phys Lett, 2007; 90: 153101 [35] Li Y S, Zhang Y, Tao N R, Lu K. Acta Mater, 2009; 57: 761 [36] Hong C S, Tao N R, Huang X, Lu K. Acta Mater, 2010; 58: 3103 [37] Zhang Y, Tao N R, Lu K. Scr Mater, 2009; 60: 211 [38] Hong C S, Tao N R, Lu K, Huang X. Scr Mater, 2009; 61: 289
Outlines

/