Abstract

Long fatigue crack propagating path in TC4ELI alloy with lamellar microstructure was studied by SEM. Statistics of angles between cracking path and α lamella exhibits that fatigue crack is apt to parallel α lamella or cross α lamella vertically, which will induce the ladder shape of crack propagating path. The parallel and vertical propagating patterns were interpreted with the weak α/β interface and the orientation of hcp α-Ti unit cell. Analysis of crack propagating path helps to understand the effect of microstructure on fatigue crack growth (FCG) rates. FCG rates tests with different microstructures reveal that in near fatigue crack threshold (ΔKth) region the thickness of α lamella is the main influential factor on fatigue crack growth rate da/dN, and the da/dN seems impervious to β grain size. However, in Paris region the FCG rates are both influenced by grain size and lamellar thickness.

Cite this article

MA Yang-Jie , LEI Jia-Feng , YANG Rui , LI Jin-Wei , TANG Zhen-Yun . INFLUENCES OF MICROSTRUCTURE ON FATIGUE CRACK PROPAGATING PATH AND CRACK GROWTH RATES IN TC4ELI ALLOY[J]. Acta Metall Sin, 2010 , 46(9) : 1086 -1092 . DOI: 10.3724/SP.J.1037.2010.00155

References

[1]Sinha V, Soboyejo W O. Mater Sci Eng A, 2001; 319-321: 607 [2]Sansoz F, Ghonem H. Mater Sci Eng A, 2003; 356: 81 [3]Lindigkeit J, Terlinde G, Gysler A, Lütjering G. Acta Metall, 1979; 27: 1717 [4]Carter R D, Lee E W, Starke E A, Beevers C. J Met Trans, 1984; 15A: 555 [5]Suresh S, Fatigue Met Trans A, 1985; 16: 249 [6]Suresh S. Translated by Wang Z G, Zang Q Sh, Li Sh X. Fatigue of Material. Beijing: Defense Industrial Press, 1999: 355 (Suresh S著, 王中光, 臧启山, 李守新译. 材料的疲劳, 北京: 国防工业出版社, 1999: 355) [7]Goswami T. Mater Design. 2003; 24: 423 [8]Ding J, Hall R, Byrne J. Int J Fatigue. 2005; 27: 1551 [9]Shademan S, Sinha V, Soboyejo A B O, Soboyejo W O. Mech of Mater, 2004; 36: 161 [10]Jata K V, Starke E A. J Met Trans A, 1986; 17A: 1011 [11]Suresh S, Zamiski G F, Ritchie R O. Met Trans A, 1981; 12A: 1435 [12]Vasudevan A K, Suresh S. Met Trans A, 1982; 13A: 2271 [13]Lütjering G. Mater Sci Eng A, 1998; 243: 32. [14]Lütjering G. Mater Sci Eng A, 1999; 263: 117 [15]Filip R, Kubiak K, Ziaja W, Sieniawski J. J Mater Processing Tech, 2003; 133: 84 [16]Li Sh K, Xiong B Q, Hui S X, Ye W J, Yu Y. Mater Sci Eng A, 2007; 460–461: 140 [17]Ma Y J, Liu J R, Lei J F, Liu Y Y, Yang R. Chinese J Mater Research, 2008; 22: 555 (马英杰, 刘建荣, 雷家峰, 刘羽寅, 杨锐. 材料研究学报, 2008; 22: 555) [18]Gil F J, Planell J A. Mater Sci Eng A, 2000; 283: 17 [19]Semiatin S L, Fagin P N, Glavicic M G, Ivasishin O M. Mater Sci Eng A, 2001; 299: 225 [20]Semiatin S L, Soper J C, Sukonnik I M. Scri Met Meterialia, 1994; 30: 951 [21]Борисова E A. Translated by Chen Sh Q. Metallography of Titanium Alloy. Beijing: Defense Industrial Press, 1986: 235 (鲍利索娃E A 著. 陈石卿译. 钛合金金相学. 北京:国防工业出版社,1986: 235). [22]Ma Y J, Liu J R, Lei J F, Liu Y Y, Yang R. Rare Met Mater Eng, 2009; 38: 976 (马英杰, 刘建荣, 雷家峰, 刘羽寅, 杨锐. 稀有金属材料与工程, 2009; 38: 976) [23]Ma Y J, Liu J R, Lei J F, Li Y R, Liu Y Y, Yang R. Acta Metall Sin, 2008; 44: 973 (马英杰, 刘建荣, 雷家峰, 李玉兰, 刘羽寅, 杨锐. 金属学报, 2008; 44: 973) [24]Ma Y J, Liu J R, Lei J F, Liu Y Y, Yang R. Rare Met Mater Eng, 2008; 37(suppl): 633 (马英杰, 刘建荣, 雷家峰, 刘羽寅,杨锐. 稀有金属材料与工程, 2008; 37(suppl): 633) [25]Xu F. PhD Thesis, Institute of Metal Research CAS, 2008 (徐峰, 博士学位论文, 中国科学院金属研究所, 2008) [26]Savage M F. Mater Sci Eng A, 2001; 319–321: 398 [27]Sansoz F, Ghonem H. Mater Sci Eng A, 2003; 356: 81 [28]Li Sh K, Xiong B Q, Hui S X, Ye W J, Yu Y. Mater Characterization, 2008; 59: 397 [29]Schroeder G, Albrecht J, Luetjering G. Mater Sci Eng A, 2001; 319–321: 602
Outlines

/

〈 〉