论文

NUMERICAL SIMULATION OF WELD POOL KEYHOLING PROCESS IN STATIONARY PLASMA ARC WELDING

  • WU Zhuan-Song
Expand
  • Key Lab for Solid–Liquid Structure Evolution and Materials Processing (Ministry of Education), Shandong University, Jinan 250061

Received date: 2010-01-11

  Revised date: 2010-04-16

  Online published: 2010-08-10

Supported by

Supported by the Key Program of National Natural Science Foundation of China (No.50936003)

Abstract

The behaviors of keyhole formation determine to a great degree the deep penetration welding process and the weld depth–width ratio in welding of medium and large thickness plates. Obtaining a deep insight into the dynamic keyholing process in the weld pool in plasma arc welding is of great significance for widening the process parameter–widow and improving the process robustness as well as weld quality stability. Based on the Level–Set theory, a numerical model is developed to describe the keyhole behaviors in the weld pool in stationary plasma arc welding (PAW), and employed to track the evolution process of keyhole boundary. In this paper, the fluid flow fields in both the plasma and the keyhole regions are constructed according to the experimental and simulation data in the previous literatures. The combined volumetric heat source model is used to numerically analyze the transient temperature field and then to determine the weld pool geometry. The algorithm of Level–Set theory combined with the transient thermal conduction model is used to determine the evolution of both keyhole and weld pool geometry at different time steps. The dynamic information on the weld pool and keyhole geometry and sizes under a few process conditions is obtained by the numerical simulation of keyholing phenomena in welding of stainless steel plates. It is found that a complete keyhole is established at 2.7 and 2.5 s for the current levels of 170 and 180 A, respectively. During the stationary PAW process, the cross–section geometry of keyhole transforms from U–shape at initial stage to V– shape later and shows finally a hyperbola shape after a complete keyhole is formed. The numerical analysis of keyhole formation is verified by measuring the efflux plasma voltage signals at the moet of keyholing.

Cite this article

WU Zhuan-Song . NUMERICAL SIMULATION OF WELD POOL KEYHOLING PROCESS IN STATIONARY PLASMA ARC WELDING[J]. Acta Metall Sin, 2010 , 46(8) : 984 -990 . DOI: 10.3724/SP.J.1037.2010.00021

References

[1] Lin S Y, Du B. Present Situation of Welding Industry and Dependent Innovation Strategy. Report of Harbin Welding Institute, 2006
(林尚扬, 杜兵. 焊接行业现状与自主创新战略. 哈尔滨焊接研究所技术报告, 2006)
[2] Lucas W. In: Japan Welding Society ed., Proc 8th Int Welding Symposium, Osaka, Japan: Japan Welding Society, 2008: 189
[3] Harwig D, Gordon R. In: Davis S A ed., Proc 6th Int Conf on Trends in Welding Research, Materials Park, Ohio: ASM International, 2003: 995
[4] Zhang Y M, Zhang S B, Jiang M. Weld J, 2002; 81: 248s
[5] Zhang Y M, Zhang S B. Weld J, 1999; 75: 53s
[6] Dong C L, Wu L, Shao Y C. China Mech Eng, 2000; 11:577
(董春林, 吴林, 邵亦陈. 中国机械工程, 2000; 11: 577)
[7] Martikainen J. J Mater Process Technol, 1995; 52: 68
[8] Keanini R G, Rubinsky B. Int J Heat Mass Transfer, 1993; 36: 3283
[9] Fan H G, Kovacevic R. J Phys, 1999; 32D: 2902
[10] Nehad A K. Int Comm Heat Mass Transfer, 1995; 22: 779
[11] Dong H G, Gao H M, Wu L. Trans China Weld Inst, 2002; 23(4): 24
(董洪刚, 高洪明, 吴林. 焊接学报, 2002; 23(4): 24)
[12] Lei Y C, Zheng H J, Chng X N. Trans China Weld Inst, 2003; 24(1): 44
(雷玉成, 郑惠锦, 程晓农. 焊接学报, 2003; 24(1): 44)
[13] Li L, Hu S S. J Tianjin Univ, 2007; 40(10): 260
(李力, 胡绳荪. 天津大学学报, 2007; 40(10): 260)
[14] Wu C S, Wang H G, Zhang M X. Acta Metall Sin, 2006; 42: 311
(武传松, 王怀刚, 张明贤. 金属学报, 2006; 42: 311)
[15] Wu C S, Wang H G, Zhang Y M. Weld J, 2006; 85: 284s
[16] Wu C S, Hu Q X, Zhang Y M. Comput Mater Sci, 2009; 46: 49
[17] Osher S, Sethian J A. J Comput Phys, 1988; 79: 12
[18] Ki H, Mohanty P S, Mazumder J. Numer Heat Transfer, 2005; 48B: 125
[19] Wu C S. Welding Thermal Processes and Molten Pool Behaviors. Beijing: China Machine Press, 2008: 106
(武传松. 焊接热过程与熔池形态. 北京: 机械工业出版社, 2008: 106)
[20] Messler Jr R W. Principles of Welding–Processes, PhysicsChemistry and Metallurgy. New York: John Wiley & Sons, Inc. 1999: 291
[21] Wang X J, Wu C S. Research Report of Institute of Materials Joining, Shandong University, 2009
(王小杰, 武传松. 山东大学材料连接研究所技术报告, 2009)

Outlines

/

〈 〉