论文

ANALYSIS OF ELECTROMAGNETIC FIELD AND JOULE HEATING OF ELECTROSLAG REMELTING PROCESSES

  • YU Fang ,
  • LI Bao-Kuan
Expand
  • School of Materials $\&$ Metallurgy, Northeastern University, Shenyang 110819

Received date: 2010-02-07

  Revised date: 2010-05-04

  Online published: 2010-07-11

Supported by

Supported by National Natural Science Foundation of China (No.50934008)

Abstract

A 3D finite element model was developed to simulate the magnetic field, electromagnetic force, current density and Joule heating of electroslag remelting< processes (electrode, slag and ingot) by using of Maxwell equation, Lorentz law and Joule law. Especially, the skin effect is shown and discussed based on numerical results. The results show that the current distribute on the external surfaces of slag and ingot. In slag, due to the low electrical conductivity of slag, the current distribution changes, gathering on the end of electrode. The maximum electromagnetic force is at the upper surface nearby the electrode and the maximum joule heating is at the interface of electrode and slag. When current frequency is greater than 35 Hz, the vortex flow  will occur in interior of electrode and ingot. When electrode immersion depth increase and slag cap thickness decrease, the maximum of the joule heat in slag will increase.

Cite this article

YU Fang , LI Bao-Kuan . ANALYSIS OF ELECTROMAGNETIC FIELD AND JOULE HEATING OF ELECTROSLAG REMELTING PROCESSES[J]. Acta Metall Sin, 2010 , 46(7) : 794 -799 . DOI: 10.3724/SP.J.1037.2010.00080

References

[1] Dong Y. J Iron Steel Res, 2007; 14(5): 7
[2] Choudhary M, Szekely J. ISS Trans, 1983; 3: 67
[3] Hernandez–Morales B, Mitchell A. Ironmaking Steelmaking, 1999; 26: 423
[4] Auburtin P. Metall Trans, 2000; 31B: 801
[5] Alghisi D, Milano M, Pazienza L. In: Morandi R ed., The 2nd Int Conf on New Developments in Metallurgical ProcessTechnology. Riva Del Garda: Association Italian Metallurgy, 2005: 19
[6] Anon J. Steel Times Int, 1997; 21(7): 20
[7] Weber V. In: Lee P D ed., The 2nd Int Conf on High Order Non–Oscillatory Methods for Wave Propagation, Transport and Flow Problems. Trento: Deutsche Forschungsgemeinschaft, 2007: 83
[8] Wei J H, Ren Y L. Acta Metall Sin, 1994; 30: 481
(魏季和, 任永莉. 金属学报, 1994; 30: 481)
[9] Wei J, Ren Y L. Acta Metall Sin, 1995; 31: 51
(魏季和, 任永莉. 金属学报, 1995; 31: 51)
[10] Geng M P, Sun D X. Process Control and Simulation in Electroslag Casting. Beijing: Metallurgical Industry Press, 2008: 47
(耿茂鹏, 孙达昕. 电渣熔铸过程控制与模拟仿真. 北京: 冶金工业出版社, 2008: 47)
[11] Patel A D. In: Gerbeth G ed., Proc 6th Int Conf on Electromagnetic Processing of Materials. Dresden: Forchungszentrum Dresden-Rossendorf, 2009: 603
[12] Patel A D. In: Peter L ed., Proc 2005 Int Symposium on Liquid Metal Processing and Casting. Ohio: ASM, 2005: 173
[13] Jardy A, Ablitzer D, Wadier J F. Metall Trans, 1991; 22B: 111
[14] Kharicha A, Sch¨utzenh¨ofer W, Ludwig A, Tanzer R, Wu M. Steel Res Int, 2008; 79: 632
[15] Bulic E, Sinigoj A R, Cestnik B. IEEE Trans Electromagnetic Compatibility, 2009; 51: 263
[16] Alghisi D, Milano M, Pazienza L. J Metall Ital, 2005; 1: 21
[17] Kawakami M, Nagata K, Yamamura M. Tetsu Hagane, 1977; 63: 2162
(川上正博, 永田和宏, 山村埝. 铁と钢, 1977; 63: 2162)

Outlines

/

〈 〉