论文

INVESTIGATION OF POST-COLD ROLLING AGING PROCESSES ON SOLUTIONIZED 7050 ALUMINUM ALLOY

  • YU Dong ,
  • MA Zong-Xi
Expand
  • Shenyang National Laboratory for Materials Science; Institute of Metal Research; Chinese Academy of Sciences; Shenyang 110016

Received date: 2009-11-02

  Revised date: 2010-02-24

  Online published: 2010-05-11

Supported by

Supported by National Basic Research Program of China (No.2005CB623708)

Abstract

7050 aluminum alloy samples were subjected to 67% cold rolling (CR) deformation after solution treatment, and then were aged at 120℃. The dislocations introduced by the CR increased the strength of the samples. The strength of the sample aged at 120℃ for 4 h (CR4) increased by 12.6% compared to that of T6 sample. The strength of the 7050 samples decreased with increasing the aging time due to the coarsening of heterogeneously--nucleated precipitates. However, the strength of the sample aged at 120 ℃ for 32 h is still higher than that of the T6 sample. Furthermore, the size and particle interval of the grain boundary precipitates increased as the aging time increased. The CR4 sample was aged at 165℃ for different times. The strength of the samples decreased with increasing the aging time due to the annihilation of dislocations and the growth of the precipitates. The strength of the sample aged at 165 ℃ for 6 h is similar to that of T76 sample. In the CR4 sample aged at 135-180℃ for 1 h, the number of dislocations reduced and the size of precipitates increased with increasing the temperature, which results in a decrease in the strength of the samples.

Cite this article

YU Dong , MA Zong-Xi . INVESTIGATION OF POST-COLD ROLLING AGING PROCESSES ON SOLUTIONIZED 7050 ALUMINUM ALLOY[J]. Acta Metall Sin, 2010 , 46(5) : 581 -588 . DOI: 10.3724/SP.J.1037.2009.00723

References

[1] Hatch J E. Aluminum Properties and Physical Metallurgy, Metals Park, Ohio: American Society for Metals, 1984: 1
[2] Wagner J A, Shenoy R N. Metall Trans, 1991; 22A: 2809
[3] Dai X Y, Xia C Q, Wu A R, Wang J W, Li Y Y. Mater Rev, 2006; 20: 104
(戴晓元, 夏长清, 吴安如, 王杰文, 李杨勇. 材料导报, 2006; 20: 104)

[4] Starink M J, Wang S C. Acta Mater, 2003; 51: 5131
[5] Dumont D, Deschamps A, Brechet Y. Mater Sci Eng, 2003; A356: 326
[6] Kamp N, Sinclair I, Starink M J. Metall Mater Trans, 2002; 33A: 1125
[7] Dixit M, Mishra R S, Sankaran K K. Mater Sci Eng, 2008; A478: 163
[8] Sha G, Cerezo A. Acta Mater, 2004; 52: 4503
[9] Wang D, Ni D R, Ma Z Y. Mater Sci Eng, 2008; A494: 360
[10] Wang D, Ma Z Y. J Alloys Compd, 2009; 469: 445
[11] Deschamps A, Brechet Y, Guyot P, Livet F. Z Metallkd, 1997; 88: 601
[12] Kassim S, Rubaie A, Barroso E K L, Godefroid L B. Int J Fatigue, 2006; 28: 934
[13] Waterloo G, Hansen V, Gjonnes J, Skjervold S R. Mater Sci Eng, 2001; A303: 226
[14] Deschamps A, Livet F, Brechet Y. Acta Mater, 1999; 47: 281
[15] Lin N A, Liu Z Y, Zeng S M. Trans Nonferrous Met Soc China, 2006; 16: 1341
[16] Zhen L, Chen J Z, Yang S J, Shao W J, Dai S L. Mater Sci Eng, 2009; A504: 55
[17] Wang D, Ma Z Y, Gao Z M. Mater Chem Phys, 2009; 117: 228
[18] Hurley P J, Humphreys F J. Acta Mater, 2003; 51: 1087
[19] Ou B L, Yang J G, Wei M Y. Metall Mater Trans, 2007; 38A: 1760
[20] Nguyen D, Thompson A W, Bernstein I M. Acta Metall, 1987; 35: 2417

Outlines

/

〈 〉