论文

EFFECT OF HIGH MAGNETIC FIELD ON THE TRANSITION BEHAVIOR OF Cu–RICH PARTICLES IN Cu–80%Pb HYPERMONOTECTIC ALLOY

  • ZHANG Lin ,
  • YU En-Gang ,
  • ZUO Xiao-Wei ,
  • SHI Ji-Cheng
Expand
  • Key Laboratory of Electromagnetic Processing of Materials; Ministry of Education; Northeastern University; Shenyang; 110004

Received date: 2009-09-21

  Revised date: 2010-01-27

  Online published: 2010-04-11

Supported by

Supported by National Natural Science Foundation of China (Nos.50574027 and 50901019), High Technology Research and Development Program of China (No.2007AA03Z519), Specialized Research Found for the Doctoral Program of Higher Education (No.20070145062), and 111 project (No.B07015)

Abstract

The Cu–80%Pb(mass fraction) hypermonotectic alloy with a dense distribution of Cu–rich particles was annealed at different temperatures under high magnetic field, the transition behavior of Cu–rich particles in solid–liquid mixture zone was investigated. The results show that, the transition behavior of Cu–rich particles occurs above 800 ℃, a compact segregation layer forms in the sample top above 900 ℃, the particle size and transition velocity increase with annealing temperature increasing. The Cu–rich particles grow and coalesce with each other during transiting, the coalescence mechanism is different from Cu–rich droplets. The clster of Cu–rich particles float up wholly, leave a clear boundary between Cu–rich particle and Cu–rich dendrite zones, the mutual interaction between the prticles makes the trnsition velocity decreased. The high magnetic field has effect on decreasing the transition velocity of Cu–rich particles, inhibiting the coarsening and coalescing of Cu–rich particles, which could decrease the segregation of Cu–rich particles, and inhibit the formation of compact Cu–rich segregation layers. Based on the mutual interaction between the particles, the acting forces on the Cu–rich particles and the final velocity have been analyzed and calculated to show the influence of magnetic field.

Cite this article

ZHANG Lin , YU En-Gang , ZUO Xiao-Wei , SHI Ji-Cheng . EFFECT OF HIGH MAGNETIC FIELD ON THE TRANSITION BEHAVIOR OF Cu–RICH PARTICLES IN Cu–80%Pb HYPERMONOTECTIC ALLOY[J]. Acta Metall Sin, 2010 , 46(4) : 423 -428 . DOI: 10.3724/SP.J.1037.2009.00629

References

[1] Dhindaw B K. Stefanescu D M, Singh A K, Curreri P A. Metall Trans, 1988; 19A: 2839
[2] Liu Y, Guo J J, Jia J, Su Y Q, Ding H S. Acta Metall Sin, 2000; 36: 1233
(刘 源, 郭景杰, 贾均, 苏彦庆, 丁宏升. 金属学报, 2000; 36: 1233)
[3] Yang S, Liu W J, Jia J. Mater Sci Technol, 2002; 10: 19
(杨森, 刘文今, 贾均. 材料科学与工艺, 2002; 10: 19)
[4] Zu D Y, Yang X H, Han X M,Wei B B. Chin J Nonferrous Met, 2003; 13: 328
(朱定一, 杨晓华, 韩秀君, 魏炳波. 中国有色金属学报, 2003; 13: 328)
[5] Yasuda H, Ohnaka I, Kawakami O, Ueno K, Kishio K. ISIJ Int, 2003; 43: 942
[6] Zhao J Z, Li H L, Wang Q L, Zhao L, He J. Acta Metall Sin, 2009; 45: 1344
(赵九洲, 李海丽, 王青亮, 赵雷, 何杰. 金属学报, 2009; 45: 1344)
[7] Ratke L, Diefenbach S. Mate Sci Eng, 1995; R15: 263
[8] Zhao J Z, Li H L, Zhao L. Acta Metall Sin, 2009; 45: 1435
(赵九洲, 李海丽, 赵雷. 金属学报, 2009; 45: 1435)
[9] Zhang L, Wang E G, Zuo X W, He J C. Acta Metall Sin, 2008; 44: 165
(张林, 王恩刚, 左小伟, 赫冀成. 金属学报, 2008; 44: 165)
[10] Xu Z M, Li T X, Zhang X P, Zhou R H. J Shanghai Jiaotong Univ, 2001; 35: 668
(许振明, 李天晓, 张雪萍, 周尧和. 上海交通大学学报, 2001; 35: 668)
[11] Zhong Y B, Ren Z M, Sun Q X, Jiang Z W, Deng K, Xu K D. Acta Metall Sin, 2003; 39: 1269
(钟云波, 任忠鸣, 孙秋霞, 江志文, 邓康, 徐匡迪. 金属学报, 2003; 39: 1269)
[12] Shu D, Sun B, Li K, hou Y. Scr Mater, 2003; 48: 1385
[13] Colli F, Fabbri M, Negrini F, Asai S, Sassa K. Int J Comput Math Electr Electron Eng, 2003; 22: 58
[14] Zhang L, Yao G C, Jiao W L. J Northeastern Univ (Nat Sci), 2004; 25: 682
(张 磊, 姚广春, 焦万丽. 东北大学学报(自然科学版), 2004; 25: 682)
[15] Zhang L. PhD Dissertation, Northeastern University, Shenyang, 2008
(张 林. 东北大学博士学位论文, 沈阳, 2008)
[16] Ratke L, Voorhees P W. Growth and Coarsening. Berlin: Springer–Verlag, 2002: 1
[17] Walter H U, Vreeburg J P B. Fluid Sciences and Materials Science in Space. Berlin: Springer–Verlag, 1987: 1
[18] Brandes E A, Brook G B. Smithells Metals Reference Book. 7th Ed., Oxford: Butterworth–Heinemann, 1998: 1
[19] Happel J. AIChE J, 1959; 5: 174
[20] Chester W. J Fluid Mech, 1957; 3: 304

Outlines

/

〈 〉