| MAGNETIC TEXTURE IN NANOCRYSTALLINESOFT MAGNETIC ALLOY |
| LIU Tao; XU Zuxiong; ZHAI Qihua; MA Ruzhang(University of Science and Technology Beijng; Beijing 100083) LUO Tong; ZHANG Chuanli(General Research Institute of Iron and Steel; Ministry of Metallurgicl Industry; Beijing 100081)(Manuscript received 1995-05-22; in revised form 1995-10-27) |
|
Cite this article:
LIU Tao; XU Zuxiong; ZHAI Qihua; MA Ruzhang(University of Science and Technology Beijng; Beijing 100083) LUO Tong; ZHANG Chuanli(General Research Institute of Iron and Steel; Ministry of Metallurgicl Industry; Beijing 100081)(Manuscript received 1995-05-22; in revised form 1995-10-27). MAGNETIC TEXTURE IN NANOCRYSTALLINESOFT MAGNETIC ALLOY. Acta Metall Sin, 1996, 32(2): 211-214.
|
|
|
Abstract Mossbauer spectroscopy was employed to investigate the magnetic texture in The nanocrystalline soft magnetic alloy Fe_(73.5)Cu_1Nb_3Si_(13.5)B_9. After crystallization a wide magnetic domain appeared obviously, which oriented preferently along the long axis of the ribbon plane and may be associated with the shape effect of the ribbon sample.(Correspondent: LIU Tao, Department of Materials Physics, University of Science and Technology Beijing,Beijing 100083)
|
|
Received: 18 February 1996
|
| 1YoshizawaY,OgumaS,YamauchiK.JApplPhys,1988;64:60442马如璋.穆斯堡尔谱学,北京钢铁学院,19843徐祖雄,马如璋,平爵云.中国科学,1985;A(1):444徐祖雄,许震东,杨会生,马如璋.科学通报,1993;38:5125StearsMB.PhysRev,1963;129:11366LiuT,zhaoZT,XuZX,MaRZ,GuoYH,CaoHM,wangYY.JApplPhys,1995;77:62147JiangJ,AubertinF,GonserU,HilzingerH-R.ZMetallk,1991;82:6988PundtA,HampelG,HesseJ.ZPhys.1992;B87:659BOHCOBCКИЙCB,著,寥莹译.铁磁学,北京:科学出版社,1965:34210HerzerG.IEEETransMagn,1990:26:139711ZbroszczykJ,CiurzynskaC,WyslockiB.JMagnMagnMater,1994;133:34712HiragaK,KohmotoO.MaterTransJIM,1991;33:86813SchaferR,HubertA,HerzerG.JApplPhys,1991;69:53252 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|