Acta Metall Sin  1996, Vol. 32 Issue (2): 211-214    DOI:
Current Issue | Archive | Adv Search |
MAGNETIC TEXTURE IN NANOCRYSTALLINESOFT MAGNETIC ALLOY
LIU Tao; XU Zuxiong; ZHAI Qihua; MA Ruzhang(University of Science and Technology Beijng; Beijing 100083) LUO Tong; ZHANG Chuanli(General Research Institute of Iron and Steel; Ministry of Metallurgicl Industry; Beijing 100081)(Manuscript received 1995-05-22; in revised form 1995-10-27)
Cite this article: 

LIU Tao; XU Zuxiong; ZHAI Qihua; MA Ruzhang(University of Science and Technology Beijng; Beijing 100083) LUO Tong; ZHANG Chuanli(General Research Institute of Iron and Steel; Ministry of Metallurgicl Industry; Beijing 100081)(Manuscript received 1995-05-22; in revised form 1995-10-27). MAGNETIC TEXTURE IN NANOCRYSTALLINESOFT MAGNETIC ALLOY. Acta Metall Sin, 1996, 32(2): 211-214.

Download:  PDF(316KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  Mossbauer spectroscopy was employed to investigate the magnetic texture in The nanocrystalline soft magnetic alloy Fe_(73.5)Cu_1Nb_3Si_(13.5)B_9. After crystallization a wide magnetic domain appeared obviously, which oriented preferently along the long axis of the ribbon plane and may be associated with the shape effect of the ribbon sample.(Correspondent: LIU Tao, Department of Materials Physics, University of Science and Technology Beijing,Beijing 100083)
Key words:  M ssbauer spectrum      nanocrystalline soft magnetic alloy      magnetic texture     
Received:  18 February 1996     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1996/V32/I2/211

1YoshizawaY,OgumaS,YamauchiK.JApplPhys,1988;64:60442马如璋.穆斯堡尔谱学,北京钢铁学院,19843徐祖雄,马如璋,平爵云.中国科学,1985;A(1):444徐祖雄,许震东,杨会生,马如璋.科学通报,1993;38:5125StearsMB.PhysRev,1963;129:11366LiuT,zhaoZT,XuZX,MaRZ,GuoYH,CaoHM,wangYY.JApplPhys,1995;77:62147JiangJ,AubertinF,GonserU,HilzingerH-R.ZMetallk,1991;82:6988PundtA,HampelG,HesseJ.ZPhys.1992;B87:659BOHCOBCКИЙCB,著,寥莹译.铁磁学,北京:科学出版社,1965:34210HerzerG.IEEETransMagn,1990:26:139711ZbroszczykJ,CiurzynskaC,WyslockiB.JMagnMagnMater,1994;133:34712HiragaK,KohmotoO.MaterTransJIM,1991;33:86813SchaferR,HubertA,HerzerG.JApplPhys,1991;69:53252
[1] MA Ruzhang; LIU Tao; CHEN Jufang; YANG Guobin; XU Zuxiong; GU Hongxia(University of Science Technology Beijing; Beijing 100083)(Manuscript received 1995-05-19). EFFECT OF YTTRIUM ADDITION ON MICROSTRUCTURE AND MAGNETIC PROPERTIES OF NANOCRYSTALLINE SOFT MAGNETIC ALLOY[J]. 金属学报, 1996, 32(2): 207-210.
[2] LIU Tao; PU Yuxie; ZHAO Zhongtao; MA Ruzhang(University of Sciene and technology Beijing; 100083). GUO Yinghuan(Institute of High Energy Physics;Chinese Academiy of Sciences;Beijing 1000800)(Manuscript received 1994-07-11;in revised form 1994-12-01). STRUCTURAL DEFECT AND INTERNAL STRESS ARRANGEMENT IN NANOCRYSTALLINE Fe73.5Cu1Nb3Si13.5B9[J]. 金属学报, 1995, 31(16): 159-163.
[3] BAI Kuichang;JIANG Ziying;HE Kaiyuan;CHENG Lizhi;ZHI Jing(Northeastern University;Shenyang)(Manuscript received 7 June;1993;in revised form 9 August;1993). STRUCTURAL STUDY OF NANOCRYSTALLINE Fe-Cu-Nb-Si-B ALLOYS BY MSSBAUER SPECTROSCOPY[J]. 金属学报, 1994, 30(14): 66-71.
No Suggested Reading articles found!