Abstract Fe-Si-B alloy has been produced from the Liaoning ludwigite by carbothermic or carbon-aluminothermic method. The effects of reducing time and temperature on B, Si and C contents in melt were investigated, and the relationship between C content and B and Si contents in melt was also discussed. The residual AI in melt was excluded by means of slag-metal equilibrium method, and the variations of Al content in melt with basicity and B and Si oxides were determined. The experimental results showed that it is feasible to produce Fe-Si-B alloy from Liaoning ludwigite and C and Al in alloy can be controlled down 0. 15% and 0.05% respectively.Correspondent: LIU Sulan, associate professor, P.O. Box 119, (Northeastern University, Shenyang 110006)
|
Received: 18 April 1996
|
1SussmanRC,EvansLG.MetallTrans,1987;18B,712鱼谷进,铃木邦辉.日本公开特许公报,昭59-118853,19843SinghalSC.USPat,4602948,19864邹元,张子青,田彦文,周继程,汪光裕.中国专利,CN1050046A,19915俞荣祥,刘素兰,冀春林.钢铁,1987;22:86梁英教,车荫昌.无机物热力学数据手册.沈阳:东北大学出版社,1993:508 |
No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
|
Shared |
|
|
|
|
|
Discussed |
|
|
|
|