Please wait a minute...
Acta Metall Sin  1996, Vol. 32 Issue (7): 763-768    DOI:
Current Issue | Archive | Adv Search |
RESEARCH ON SURFACE FILMS FORMED BY 5454 Al-Mg ALLOY TUBE AND PURE ALUMINIUM TUBE IN CARBONATED SOLUTION
FANG Yaohua; ZHANG Mingjie(Nanjing University of Chemical Technology; Nan jing 210009);SUN Yuzhen; WANG Wenhao (Institute of Metal Research; Chinese Academy of Sciences; Shenyang 110015)(Manuseript received 1995-12-15)
Cite this article: 

FANG Yaohua; ZHANG Mingjie(Nanjing University of Chemical Technology; Nan jing 210009);SUN Yuzhen; WANG Wenhao (Institute of Metal Research; Chinese Academy of Sciences; Shenyang 110015)(Manuseript received 1995-12-15). RESEARCH ON SURFACE FILMS FORMED BY 5454 Al-Mg ALLOY TUBE AND PURE ALUMINIUM TUBE IN CARBONATED SOLUTION. Acta Metall Sin, 1996, 32(7): 763-768.

Download:  PDF(404KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The surface films respectively formed by 5454 Al-Mg alloy tube and pure aluminium tube in carbonated solution were studied using AES, XPS, SIMS and CWT. The results show that the main composition of the surface film is hydrated oxide of aluminium.The thinner the surface film is, the better corrosion resistance behaviour it has. The intensification of magnesium results in the better anti-corrosion property of the alloy than that of pure aluminium. The content of magnesium ions in the surface film is two orders of magnitude higher than that in the inner matrix.Correspondent: FANG Yaohua, associate professor, Department of Applied Chemistry, Nanjing University of Chemical Technology. Nanjing 210009
Key words:  surface film      Al-Mg alloy tube      carbonated solution      corrosive wear     
Received:  18 July 1996     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1996/V32/I7/763

1于福洲.金属材料的耐腐蚀性.北京:科学出版社,1982:3502 陆家和,陈长彦.表面分析技术.北京:电子工业出版社,1987:2003 WagnerCD,RiggsWM,DavisLE,MoulderJF.HandbookofX-RayPhotoelectronSpectroscopyEdenPrairie,Minnesota:PhysicalElectronicsDivision,Perkin-ElmerCorporation,1979:4
[1] Jinhui LIU, Yingwei SONG, Dayong SHAN, En-Hou HAN. Comparative Study on Corrosion Behavior of Cast and Forged Mg-5Y-7Gd-1Nd-0.5Zr Alloys[J]. 金属学报, 2018, 54(8): 1141-1149.
[2] WANG Xianfei, XIONG Shoumei. USE OF SO2/AIR/N2 COVER GASES FOR THE PROTECTION ON MOLTEN MAGNESIUM AND AZ91D ALLOY[J]. 金属学报, 2014, 50(1): 32-40.
[3] WANG Xianfei XIONG Shoumei. CHARACTERIZATION OF THE SURFACE FILM FORMED ON MOLTEN AZ91D MAGNESIUM ALLOY PROTECTED BY SO2 MIXTURES[J]. 金属学报, 2010, 46(12): 1529-1533.
[4] WANG Jihui; JIANG Xiaoxia; LI Shizhuo (Institute of Metal Research; The Chinese Academy of Sciences; Shenyang 110015). CORROSIVE WEAR BEHAVIOR OF COPPER ALLOYS IN 3.5% NaCl+NH_3(NH_4~+) SOLUTION[J]. 金属学报, 1997, 33(12): 1268-1274.
[5] BI Hongyun; JIANG Xiaoxia; LI Shizhuo;YANG Jingxian(Institute of Metal Research; Chinese academy of Sciences; Shenyang 110015)(Shenyang Polytechnic University; Shenyang 110023). THE CORROSIVE WEAR BEHAVIOR OF Cr-Mn-N SERIES CASTING STAlNLESS STEEL[J]. 金属学报, 1997, 33(10): 1069-1074.
[6] HUANG Yanliang; JIANG Xiaoxia; LI Shizhuo (Institute of Metal Research; Chinese Academy of Sciences; Shenyang 110015)(Manuscript received 1995-03-13; in revised form 1995-07-01). CORROSIVE WEAR OF STAINLESS STEEL IN Cl~-+H_2SO_4 SOLUTION UNDER LOW LOADS[J]. 金属学报, 1996, 32(1): 57-62.
[7] LU Hinchun;LI;ZHANG Tiancheng;JIANG Hiaoxia(Institute of Metal Research;Chinese Academy of Sciences;Shenyang)(Manuscript received 5 August;1993;in revised form 18 October;1993). EFFECT OF SOLUTION ANNEALING TEMPERATURE ON CORROSIVE WEAR BEHAVIOUR OF DUPLEX STAINLESS STEEL IN SULPHURIC ACID MEDIUM[J]. 金属学报, 1994, 30(16): 159-164.
[8] JIANG Xiaoxia;LI Shizhuo;SHI Changxu Institute of Metal Research; Academia Sinica; ShenyangZHANG Tiancheng;Institute of Metal Research;Academia Sinica;Shenyang 110015. INTERACTION BETWEEN CORROSION AND WEAR OF STAINLESS STEEL IN H_3PO_4 + NaCl SOLUTION[J]. 金属学报, 1993, 29(5): 74-79.
[9] JIANG Xiaoxia;SUN Li;LI Shizhuo;XIAO Yaotian Institute of Metal Research; Academia Sinica; Shenyang. CORROSIVE WEAR BEHAVIOUR OF CD-4MCu ALLOY IN PHOSPHORIC ACID MEDIA[J]. 金属学报, 1992, 28(2): 59-63.
[10] JIANG Xiaoxia;LI Shizhuo Institute of Metal Research; Academia Sinica; Shenyang. LIN Xiaopin;YANG Jingxiang Shenyang University of Technology. CORROSIVE WEAR PERFORMANCE OF STAINLESS STEELS IN DILUTE ACIDIC MEDIA[J]. 金属学报, 1991, 27(1): 98-101.
No Suggested Reading articles found!