| EXPERIMENTAL AND THEORETICAL STUDY ON NON-LINEAR ANELASTIC INTERNAL FRICTION |
| GE Tingsui (T S. KE); (Laboratory of Internal Friction and Defects in Solinds; Institute of Solid State Physics; Chinese Academy of Sciences; Hefei 230031) |
|
Cite this article:
GE Tingsui (T S. KE); (Laboratory of Internal Friction and Defects in Solinds; Institute of Solid State Physics; Chinese Academy of Sciences; Hefei 230031). EXPERIMENTAL AND THEORETICAL STUDY ON NON-LINEAR ANELASTIC INTERNAL FRICTION. Acta Metall Sin, 1997, 33(1): 9-21.
|
|
|
Abstract A critical review is made on the recent development of the research on non-linear anelastic internal friction. The chief difference between the non-linear anelastic internal friction and its linear counter part is that in the linear case only internal friction peaks versus temperature and versus frequency appear, whereas in the non-linear case appears also internal friction peak versus strain amplitude within the temperature region of the internal friction peak versus temperature,Since the discovery of the non-linear anelastic internal friction in 1950, two systems exhibitiing non-linear anelastic internal frictions have been found and investigated: (1) The interacti0n between point defects (vacancies and solute atoms) and dislocations. A series of experimental results have been obtained concerning this subject, appropriate physical models have been suggested and priliminary theoretical analysis have been attached. (2) The interaction between dislocation and grain boundaries (bamboo grain boundary and bicrystals). Some experimental results have been obtained concerening which further experimental and theoretical studies are requird.
|
|
Received: 18 January 1997
|
1Ke T S.Phys Rev,1950;78:420,J Alloys Compounds,1994;211/212:290,金属学报,1980;16:218 2葛庭燧.自然科学进展,1995; 5:521,Phys Status Solidi(a),1996物理学批 1996 3葛庭燧,方前锋.自然科学进展,1996 4方前锋,葛庭燧.自然科学进展,1996 5 Ke T S.Phys Rev,1947 71:533 6葛庭燧。力学进展,1993;23(8):289, Mater Sci Eng,1994;A186:1 7 Ke T S,Cui P,Guan X S. Scr Metall Mater,1992;27:1151 8Ke T S Chen P P Phys Status Solidi(a),1995;148:439 9 Yuan L Y, Ke T S Scr Metall Mater,1996 10 Ke T S,Duan Yuhua.Acta Metall Mater,1993;4:1003,Phys StatusSolidi(a),1993;140:411 11 Guan X S Ke T S J Alloys Compounds,1994;211/212:480 12 Chen Zhiying,Duan Yuhua,Ge Tingsui(Ke T S)Acta Mech Sin 1995;11:259 13 Ke T S.J Appl Phys,1949;20:274 |