EFFECTS OF CRYSTAL ORIENTATION AND LOAD MODE ON FATIGUE BEHAVIOR IN Ni_3Al ALLOY SINGLE CRYSTALS
ZHANG Guangping;WANG Zhongguang (State Key Laboratory for Fracture and Fatigue of Materials; Institute of Metal Research; Chinese Academy of Sciences;Shenyang 110015)
Cite this article: 

ZHANG Guangping;WANG Zhongguang (State Key Laboratory for Fracture and Fatigue of Materials; Institute of Metal Research; Chinese Academy of Sciences;Shenyang 110015). EFFECTS OF CRYSTAL ORIENTATION AND LOAD MODE ON FATIGUE BEHAVIOR IN Ni_3Al ALLOY SINGLE CRYSTALS. Acta Metall Sin, 1997, 33(10): 1009-1014.

Download:  PDF(2485KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  Fatigue tests under nominal I and mixed modeⅠ/ Ⅱ loading were carried out on Ni3Al alloy single crystals. The effects of crystal orientation and load mode on the fatigue cracking behavior were studied. It was found that the crack paths are dependent on both crystal orientation and applied load mode. Fatigue cracking in single crystals under mixed mode Ⅰ/ Ⅱ loading always occurs on the planes with maximum resolved shear stress rather than on those with maximum normal stress. The cracking behavior predicted by main mixed mode criteria in polycrystalline materials under a mixed mode can be explained from the present results.
Key words:  crystal orientation      mixed mode loading      Ni_3Al alloy single crysta1      fatigue cracking     
Received:  18 October 1997     

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1997/V33/I10/1009

1 Westbrook J H Trans Metall Soc AIME.1957:209:898
2 Flinn P A,Trans Metall Soc AIME 1960;218:145
3 Copley S M, Kear B H. Trans Metall Soc AIME,1967 239:977
4 Zhang G P,Wang Z G,Li G Y Acta Metall Mater,1997;45:1705
5 Kuruvilla A K,Stoloff N S.Scr metall ,1987;21:873
6 Matuszyk W,Camus G,Duquete D J,Stoloff N S ,Metall Trans,1990;21A:2967
7 Paris P C,Sih G C .ASTM STP 381,1965;30
8 Peach M D,Kochler J S Phys Rev,1950;80:436
9 Erdogan F,Sih G C .J Basic Eng.1963;85:519
10 Sih G C.Int J Fracture, 1974;10:305
11 Hussain M A、 Pu S L, Underwood J. ASTM STP 560,1974:2
[1] LIU Jinlai, YE Lihua, ZHOU Yizhou, LI Jinguo, SUN Xiaofeng. Anisotropy of Elasticity of a Ni Base Single Crystal Superalloy[J]. 金属学报, 2020, 56(6): 855-862.
[2] SUN Heng,LIN Xiaoping,ZHOU Bing,ZHAO Shengshi,TANG Qin,DONG Yun. Microstructures and Tensile Deformation Behavior of Directionally Solidified Mg-xGd-0.5Y Alloys[J]. 金属学报, 2020, 56(3): 340-350.
[3] HU Bin,LI Shusuo,PEI Yanling,GONG Shengkai,XU Huibin. Influence of Small Misorientation from <111> on Creep Properties of a Ni-Based Single Crystal Superalloy[J]. 金属学报, 2019, 55(9): 1204-1210.
[4] Li WANG,Zhongjiao ZHOU,Shaohua ZHANG,Xiangdong JIANG,Langhong LOU,Jian ZHANG. CRACK INITIATION AND PROPAGATION AROUND HOLES OF Ni-BASED SINGLE CRYSTAL SUPERALLOY DURING THERMAL FATIGUE CYCLE[J]. 金属学报, 2015, 51(10): 1273-1278.
[5] LIU Fencheng, LIN Xin, YU Xiaobin, HUANG Chunping, HUANG Weidong. EVOLUTION OF INTERFACE AND CRYSTAL ORIENTATION OF LASER SOLID FORMED GH4169 SUPERALLOY DURING RECRYSTALLIZATION[J]. 金属学报, 2014, 50(4): 463-470.
[6] ZHANG Zhefeng ZHANG Peng TIAN Yanzhong ZHANG Qingke QU Shen ZOU Hefei DUAN Qiqiang LI Shouxin WANG Zhongguang. INTERFACIAL EFFECTS OF FATIGUE CRACKING IN METALLIC MATERIALS[J]. 金属学报, 2009, 45(7): 788-800.
[7] JIA Yuxian JIN Tao LIU Jinlai SUN Xiaofeng HU Zhuangqi. ANISOTROPIC CREEP IN A Ni-BASED SINGLE CRYSTAL SUPERALLOY[J]. 金属学报, 2009, 45(11): 1364-1369.
[8] HU Yunming;WANG Zhongguang(State Key Laboratory for Fatigue and Fracture of Materials; Institute of Metal Research; The Chinese Academyof Sciences; Shenyang 110015)Correspondent; HU Yunming; Tel: (024)23843531-55gg5; Fax: (024)23891s20Manuscript received 1997-12-17; in revised form 1998-01-30. CYCLIC DEFORMATION BEHMIOR AND FATIGUE CRACK INITIATION IN COPPER BICRVSTALS[J]. 金属学报, 1998, 34(12): 1255-1260.
[9] WU Donghai;HU Gengxiang (Department of Materials Science; Shanghai Jiaotong University; Shanghai 200030)INUI Haruyuki; YAMAGUCHI Masaharu (Kyoto University; Kyoto 606-01; Japan). DEFORMATION BEHAVIOR OF γ-TiAl SINGLE CRYSTALS AT DIFFERENT TEMPERATURES[J]. 金属学报, 1998, 34(1): 39-44.
[10] ZHANG Guangping; WANG Zhongguang; LI Guangyi (State Key laboratory for Fracture and Fatigue of Materials; Institute of Metal Research; Chinese Academy of Sciences; Shenyang 110015). FATIGUE CRACKING IN Ni3Al SINGLE CRYSTAL UNDER CYCLIC COMPRESSIVE LOAD[J]. 金属学报, 1996, 32(11): 1149-1153.
[11] HE Guo;LI Jianguo;MAO Hiemin;FU Hengzhi(Northwestern Polytechnical University;Hi'an 710072)(Manuscript received 1994-09-13.in revised form 1995-03-13). INFLUENCE OF CRYSTAL ORIENTATION ON THE PRIMARY DENDRITE ARM SPACING OF A SINGLE CRYSTAL SUPERALLOY[J]. 金属学报, 1995, 31(7): 309-314.
[12] WANG Li; CHEN Lian(Institute of Metal Research; Chinese Academy of Sciences;Liaoning Key Laboratory for Materials and Hydrogen;Shenyang 110015)(Manuscript recieved 1994-06-25; in revised form 1995-01-16). DOUBLE PEAK OF HYDROGEN ACCUMULATION NEAR NOTCH TIP UNDER Ⅰ+Ⅱ LOADING MODE[J]. 金属学报, 1995, 31(10): 461-468.
[13] XIA Yuebo; ZHANG Tianyi (State Key Laboratory for Fracture and Failure of Materials; Institute of Metal Research; Academia Sinica; Shenyang) DENG Jun (Shenyang Polytechnical University). EFFECT OF ORIENTATION ON STRESS RESPONSE, FRICTION STRESS AND BACK STRESS DURING CYCLIC DEFORMATION IN AI SINGLE CRYSTALS.[J]. 金属学报, 1992, 28(8): 42-48.
[14] GAO Hua;CHEN Youxuan;LI Ming;CHEN Dehai Shanghai University of Engineering Science Shanghai Dalong Machinery associate professor;Department of Materials;Shanghai University of Engineering Science;Shanghai 200051. EFFECT OF NON-PROPORTIONAL OVERLOADINGON FATIGUE CRACK GROWTH[J]. 金属学报, 1990, 26(4): 66-72.
[15] JIN Nengyun Shanghai Jiaotong University. CYCLIC DEFORMATION OF FCC CRYSTALS AND ITS DISLOCATION INTERACTION MODEL Ⅰ. CYCLIC DEFORMATION OF COPPER SINGIE CRYSTALS[J]. 金属学报, 1988, 24(5): 299-310.
No Suggested Reading articles found!