| CORROSIVE WEAR BEHAVIOR OF COPPER ALLOYS IN 3.5% NaCl+NH_3(NH_4~+) SOLUTION |
| WANG Jihui; JIANG Xiaoxia; LI Shizhuo (Institute of Metal Research; The Chinese Academy of Sciences; Shenyang 110015) |
|
Cite this article:
WANG Jihui; JIANG Xiaoxia; LI Shizhuo (Institute of Metal Research; The Chinese Academy of Sciences; Shenyang 110015). CORROSIVE WEAR BEHAVIOR OF COPPER ALLOYS IN 3.5% NaCl+NH_3(NH_4~+) SOLUTION. Acta Metall Sin, 1997, 33(12): 1268-1274.
|
|
|
Abstract The corrosion rate, corrosive wear rate and polarization curves of aluminium brass and cupronickel alloy were determined in 3.5%NaCl and 3.5%NaCl+NH3(NH4+)solutions, the wear tracks of copper alloys were observed by SEM, the specific energy of the surface layer after corrosion was also measured by single pendulum scratching test. Experimental results show that the addition of ammonia or ammonium in 3.5%NaCl solution can accelerate the corrosion and corrosive wear of copper alloys, the corrosion potential shifts negativly,the corrosion current density increases. The ammonia or ammonium caused the surface embrittlement of copper alloys during corrosive wear.
|
|
|
1北京电力试验研究所化学室.北京电力技术,1979;2-3:87 2王杏卿.热力设备的腐蚀与防护.北京:水利电力出版社,1989:247 3化学工业部化工机械研究院.腐蚀与防护手册.北京:化学工业出版社,1989:121 4肖纪美.腐蚀总论──材料的腐蚀及其控制方法.北京:化学工业出版社,1994:77 5张天成,姜晓霞,路新春,李诗卓.中国腐蚀与防护学报,1994;14:297 6姜晓霞,张天成,李诗卓,史亦农材料保护,1995;28(1):1 7梁亚南.中国科学院金属研究所博士学位论文,1995 8张天成,姜晓霞,路新春,李诗卓.材料研究学报,1994; 8:397 9Macdonald D D, Syrett B C, Wings S. Corrosion, 1979; 35: 367 10Beccaria A M,Poggi G,Traverso P,Ghiazza M.Corros Sci,1991;32:1163| |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|