CORROSIVE WEAR BEHAVIOR OF COPPER ALLOYS IN 3.5% NaCl+NH_3(NH_4~+) SOLUTION
WANG Jihui; JIANG Xiaoxia; LI Shizhuo (Institute of Metal Research; The Chinese Academy of Sciences; Shenyang 110015)
Cite this article: 

WANG Jihui; JIANG Xiaoxia; LI Shizhuo (Institute of Metal Research; The Chinese Academy of Sciences; Shenyang 110015). CORROSIVE WEAR BEHAVIOR OF COPPER ALLOYS IN 3.5% NaCl+NH_3(NH_4~+) SOLUTION. Acta Metall Sin, 1997, 33(12): 1268-1274.

Download:  PDF(1387KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The corrosion rate, corrosive wear rate and polarization curves of aluminium brass and cupronickel alloy were determined in 3.5%NaCl and 3.5%NaCl+NH3(NH4+)solutions, the wear tracks of copper alloys were observed by SEM, the specific energy of the surface layer after corrosion was also measured by single pendulum scratching test. Experimental results show that the addition of ammonia or ammonium in 3.5%NaCl solution can accelerate the corrosion and corrosive wear of copper alloys, the corrosion potential shifts negativly,the corrosion current density increases. The ammonia or ammonium caused the surface embrittlement of copper alloys during corrosive wear.
Key words:  copper alloys      corrosive wear      ammonia(ammonium)     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1997/V33/I12/1268

1北京电力试验研究所化学室.北京电力技术,1979;2-3:87
2王杏卿.热力设备的腐蚀与防护.北京:水利电力出版社,1989:247
3化学工业部化工机械研究院.腐蚀与防护手册.北京:化学工业出版社,1989:121
4肖纪美.腐蚀总论──材料的腐蚀及其控制方法.北京:化学工业出版社,1994:77
5张天成,姜晓霞,路新春,李诗卓.中国腐蚀与防护学报,1994;14:297
6姜晓霞,张天成,李诗卓,史亦农材料保护,1995;28(1):1
7梁亚南.中国科学院金属研究所博士学位论文,1995
8张天成,姜晓霞,路新春,李诗卓.材料研究学报,1994; 8:397
9Macdonald D D, Syrett B C, Wings S. Corrosion, 1979; 35: 367
10Beccaria A M,Poggi G,Traverso P,Ghiazza M.Corros Sci,1991;32:1163|
[1] BI Hongyun; JIANG Xiaoxia; LI Shizhuo;YANG Jingxian(Institute of Metal Research; Chinese academy of Sciences; Shenyang 110015)(Shenyang Polytechnic University; Shenyang 110023). THE CORROSIVE WEAR BEHAVIOR OF Cr-Mn-N SERIES CASTING STAlNLESS STEEL[J]. 金属学报, 1997, 33(10): 1069-1074.
[2] FANG Yaohua; ZHANG Mingjie(Nanjing University of Chemical Technology; Nan jing 210009);SUN Yuzhen; WANG Wenhao (Institute of Metal Research; Chinese Academy of Sciences; Shenyang 110015)(Manuseript received 1995-12-15). RESEARCH ON SURFACE FILMS FORMED BY 5454 Al-Mg ALLOY TUBE AND PURE ALUMINIUM TUBE IN CARBONATED SOLUTION[J]. 金属学报, 1996, 32(7): 763-768.
[3] HUANG Yanliang; JIANG Xiaoxia; LI Shizhuo (Institute of Metal Research; Chinese Academy of Sciences; Shenyang 110015)(Manuscript received 1995-03-13; in revised form 1995-07-01). CORROSIVE WEAR OF STAINLESS STEEL IN Cl~-+H_2SO_4 SOLUTION UNDER LOW LOADS[J]. 金属学报, 1996, 32(1): 57-62.
[4] LU Hinchun;LI;ZHANG Tiancheng;JIANG Hiaoxia(Institute of Metal Research;Chinese Academy of Sciences;Shenyang)(Manuscript received 5 August;1993;in revised form 18 October;1993). EFFECT OF SOLUTION ANNEALING TEMPERATURE ON CORROSIVE WEAR BEHAVIOUR OF DUPLEX STAINLESS STEEL IN SULPHURIC ACID MEDIUM[J]. 金属学报, 1994, 30(16): 159-164.
[5] JIANG Xiaoxia;LI Shizhuo;SHI Changxu Institute of Metal Research; Academia Sinica; ShenyangZHANG Tiancheng;Institute of Metal Research;Academia Sinica;Shenyang 110015. INTERACTION BETWEEN CORROSION AND WEAR OF STAINLESS STEEL IN H_3PO_4 + NaCl SOLUTION[J]. 金属学报, 1993, 29(5): 74-79.
[6] JIANG Xiaoxia;SUN Li;LI Shizhuo;XIAO Yaotian Institute of Metal Research; Academia Sinica; Shenyang. CORROSIVE WEAR BEHAVIOUR OF CD-4MCu ALLOY IN PHOSPHORIC ACID MEDIA[J]. 金属学报, 1992, 28(2): 59-63.
[7] JIANG Xiaoxia;LI Shizhuo Institute of Metal Research; Academia Sinica; Shenyang. LIN Xiaopin;YANG Jingxiang Shenyang University of Technology. CORROSIVE WEAR PERFORMANCE OF STAINLESS STEELS IN DILUTE ACIDIC MEDIA[J]. 金属学报, 1991, 27(1): 98-101.
No Suggested Reading articles found!