| STUDY ON α/γ PHASE EQUILIBRIUM IN Ti-Al-Cr-Fe QUARTERNARY SYSTEM |
| LI Juntao; HAO Shiming; WAN Qingfeng (Department of Materials Science and Engineering; Northeastern University; Shenyang 110006)Correspondent: HAO Shiming; professor; Tel: (024)23893000-7737; E-mail: smhao@mail. neu. eds. cn |
|
Cite this article:
LI Juntao; HAO Shiming; WAN Qingfeng (Department of Materials Science and Engineering; Northeastern University; Shenyang 110006)Correspondent: HAO Shiming; professor; Tel: (024)23893000-7737; E-mail: smhao@mail. neu. eds. cn. STUDY ON α/γ PHASE EQUILIBRIUM IN Ti-Al-Cr-Fe QUARTERNARY SYSTEM. Acta Metall Sin, 1998, 34(9): 897-902.
|
|
|
Abstract A simple type of diffusion couple was designed. The compositions of the phase equilibrium α/γ at 1200℃ and 1250℃ in Ti-Al-Cr-Fe quarternary system have been determined by the diffusion couple-electron probe method, and partial isothermal squares for Ti-Al-Cr-Fe quarternary system have been drawn. The results show that Cr has the effect of increasing the solubility for Fe in the α phase and Fe has the effect of increasing the solubility for Cr in the α phase.
|
|
Received: 18 September 1998
|
1 Kim Y W .JOM, 19895 41(7):24 2 Kim Y W JOM,1994;46(7):30 3 山口正治,乾晴行,日井泰治金属,1995;65:215(Yamaguchi M, Inui H; Shiroi T, Met Technol, 1995; 65: 215) 4 桥本健纪,土肥春夫,还本得藏,铃木朝夫日本金属学会志,1988;52(8):816(Hashimoto K,Doi H,Kasahara K;Tsujimoto T,SuzukiT.J Jpn Inst Met,19882 52:816) 5 Nakagawa Y G, Yokoshima S, Matsuda K. Mate, Sci Eng, 1992; A153: 722 6 丁进军,赵刚,郝士明金属学报,19972 33:1105(Ding J J, Zhao G, Hao S M. Acta Metall Sinica, 1997 33: 1105) 7 李俊涛,郝士明东北大学学报,1997;18:362(Li J T, Hao S M. J Northeastern University, 1997 18: 362) 8 蒋敏,郝士明中国物理协会第六届全国相图学术会议论文集,1990:150(Jiang M,HaoS M.Proceedings of the 6th NationalSymposium on Phase Diagrams, Commission on Phase Diagrams of the Chinese Physical Societyl1990:150) 9 丁进军,赵刚,蒋敏,郝士明材料研究学报, 1998(in Press)(Ding J J, Zhao G, Jian M. Chin J Mat Res, 1998(in press))A |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |