WANG Huabin; HAN Jiecai; ZHANG Xinhong; DU Shanyi (Center for Composite Materials; Harbin Institute of Technology; Harbin 150001)Correspondent: WANG Huabin; lecturer;Tel: (0451)6414167; Fax: (0451)6415605. REACTION MECHANISM OF CONTINUALLY HEATING Ni AND A1 PARTICLES. Acta Metall Sin, 1998, 34(9): 992-998.
Abstract There are three exothermic peaks and two endothermic peaks in Ni-Al differential thermal analysis (DTA) curves. Three exothermic peaks are respectively attributed to NiAl3 formation by solid-solid diffusion of Ni and Al power, Ni2Al3 formation by liquid eutectic spreading on the surface of Ni power, and Ni2Al3 and NiAl formation by diffusion. Two endothermic peaks are respectively caused by primary eutectic contact melting and later A1 melting, and anti-peritectic reaction of NiAl3.
1NaiborodenkoY S, Itin V I. CombustExplos Shock Wave(USSR), 1975; 11: 626 2 Anselmi-Tamburini U, Munir Z A.J Appl Phys, 1990; 66: 5033 3Rogochev A S, Varma A, Merzhanov A G. Int J SHS ,1993; 2: 25 4 Rogochev A S, Khomenko I O, Varma A, Mezhanov A G, Ponomarev. Int J SHS, 1994; 3: 239 5 Philpot K A, Munir Z A, Holt J B.J Mater Sci, 1987; 22: 159 6 Colgon E G. Mate, Sci Rep, 1990; 5: 1 7王华彬,韩杰才,杜善义金属学报,1998;34:461(Wang H B, Han J C, Du S Y. Acta Metall Sin, 1998; 34: 461)g