Please wait a minute...
Acta Metall Sin  1998, Vol. 34 Issue (9): 999-1004    DOI:
Current Issue | Archive | Adv Search |
THE ENHANCEMENT OF FLUX PINNING PROPERTIES OF (BiPb)_2Sr_2Ca_2Cu_3O(10+δ) WITH ADDITION OF NANO-SiC
SU Xiaodong;YANG Zongquan; WANG Yongzhong;ZHANG Cheng; HUA Ling; TANG Hong;QIAO Guiwen (Institute of Metal Research; The Chinese Academy of Sciences; Shenyang 110015)Correspondent: SU Xiaodong; Tel: (024)25843531-55842; E-mail: xdsu@imr.ac.cn
Cite this article: 

SU Xiaodong;YANG Zongquan; WANG Yongzhong;ZHANG Cheng; HUA Ling; TANG Hong;QIAO Guiwen (Institute of Metal Research; The Chinese Academy of Sciences; Shenyang 110015)Correspondent: SU Xiaodong; Tel: (024)25843531-55842; E-mail: xdsu@imr.ac.cn. THE ENHANCEMENT OF FLUX PINNING PROPERTIES OF (BiPb)_2Sr_2Ca_2Cu_3O(10+δ) WITH ADDITION OF NANO-SiC. Acta Metall Sin, 1998, 34(9): 999-1004.

Download:  PDF(1169KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The influences of nano-SiC on the superconducting properties of Bi2223, especially on the flux pinning have been studied by using XRD, SEM, SQUID, VSM. The results reveal that the nano-particles of SiC do not change the transition temperature obviously. The magnetization areas on the M - H curve, intragranular critical density Jcm and average flux pinning force Fp were improved due to proper amount of nano-SiC addition at temperature 5 K and 77 K. According to these evidences, we can infer that the nano-SiC particles introduced and homogenuosly dispersed in superconducting matrice take the role of effective flux pinning centers.
Key words:  nano-SiC      Bi2223 superconductor      flux pinning     
Received:  18 September 1998     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1998/V34/I9/999

1 Hikata T, Nichikaw T, Mukai H, Sato K, Hiotsuyanayi M. Jpn J Appl Phys, 1989; 28: 288
2 Dou S X, Liu H K, Wang J, Apperlay M H, Sorrell C C, Guo S J, Loberg B, Easterling R E. Physica C 1990;172: 63
3 Heine K, Tenbrink J, Thoner M. Appl Phys Lett, 1989; 55: 2441
4 Murakami M, Gotoh S, Fuimoto H, Yamaguchi K, Koshisuga N, Tanaka S. Physica C 1991; 321: 185
5 Zhang Q R. High Temperature Superconductivity. Zhejiang University Press, 1992: 435
6 Su X D, Yang Z Q, Wang Y Z, Tong H, Zhang C, Hua L, Qiao G W. Phhsica C 1997; 282-287: 1615
7 Yang Peidong, Lieber C M. Science, 1996; 273: 1836
8 Bean P. Phys Rev Lett, 1962; 8: 250
9 Bean P J Appl Phys, 1962; 33: 3334
10 Bean P. Rev Mod Phys, 1964; 31: 36
11 Ginsberg D M. Physical Properties of High Temperature Superconductors. World Sciences Press,1989: 87
No related articles found!