| [1] Huang J T. Theory and Application of Cavitation and Cavitation Erosion. Beijing: Tsinghua University Press, 1991: 113
(黄继汤. 空化与空蚀的原理及应用. 北京: 清华大学出版社, 1991: 113)
[2] Tomita Y. Shock Wave Science and Teschnology Reference Library. Heidelberg: Springer, 2007: 37
[3] Berchiche N, Franc J P, Michel J M. J Fluids Eng, 2002; 124: 601
[4] Okada T, Iwai Y, Hattori S, Tanimura N.Wear, 1995; 184:231
[5] Bedkowsi W, Gaisiak G, Lachowicz C. Wear, 1999; 230:201
[6] Paulo V M, Roseana E T. Mater Charact, 1998; 41: 193
[7] Jiang S L, Zheng Y G, Yao Z M. Corros Sci, 2006; 48:2614
[8] Liu W, Zheng Y G, Yao Z M, Wu X Q, Ke W. Acta Metall Sin, 2001; 37: 197
(柳 伟, 郑玉贵, 姚治铭, 吴欣强, 柯 伟. 金属学报, 2001; 37: 197)
[9] Luo S Z, Jing H M, Zheng Y G, Yao Z M, Ke W. J ChinSoc Corros Prot, 2003; 23: 206
(骆素珍, 敬和民, 郑玉贵, 姚治铭, 柯 伟. 中国腐蚀与防护学报, 2003; 23: 206)
[10] Wang Z Y, Chen H P, Xu Y G, Zhu J H. J Xi’an JiaotongUniv, 2002; 36: 744
(王再友, 陈黄浦, 徐英鸽, 朱金华. 西安交通大学学报, 2002; 36: 744)
[11] Liu W, Zheng Y G, Liu C S, Yao Z M, Ke W. Acta Metall Sin, 2003; 39: 85
(柳伟, 郑玉贵, 刘常升, 姚治铭, 柯伟. 金属学报, 2003; 39: 85)
[12] Luo S Z, Jing H M, Zheng Y G, Yao Z M, Ke W. J ChinSoc Corros Prot, 2003; 23: 276
(骆素珍, 敬和民, 郑玉贵, 姚治铭, 柯伟. 中国腐蚀与防护学报, 2003; 23: 276)
[13] Luo S Z, Zheng Y G, Jiang S L, Yao Z M, Ke W. CorrosSci Prot Technol, 2004; 16: 352
(骆素珍, 郑玉贵, 蒋胜利, 姚治铭, 柯 伟. 腐蚀科学与防护技术, 2004; 16: 352)
[14] Ren Y S, Wang Y M, Liu J Y, Qu J X. Met Heat Process,2003; 28(8): 20
(任玉锁, 王义民, 刘俊英, 曲敬信. 金属热处理, 2003; 28(8): 20)
[15] Chen H S, Liu S H, Wang J D, Chen D R. J Appl Phys,2007; 101: 103510
[16] ASTM G32–92, Standard Method of Vibratory Cavitation Erosion Test. Annual Book of ASTM Standards, Vol.03.02, Philadelphia, PA: ASTM, 1995
[17] Chen H S, Li J, Chen D R, Wang J D. Wear, 2008; 265:692
[18] Xue W, Chen Z Y. Mater Mech Eng, 2005; 29(2): 59
(薛伟, 陈昭运. 机械工程材料, 2005; 29(2): 59)
[19] Meyers M A, translated by Zhang Q M, Liu Y, Huang F L,Lu Z J. Dynamic Behavior of Materials. Beijing: National Defense Industry Press, 2006: 16
(Meyers M A著, 张庆明, 刘 彦, 黄风雷, 吕中杰译. 材料的动力学行为. 北京: 国防工业出版社, 2006: 16) |