EFFECT OF COLD ROLLING AND ANNEALING ON THE TEXTURE OF Ti-18Nb-4Sn ALLOY
YOU Li
北京科技大学新金属材料国家重点实验室
Cite this article: 

YOU Li. EFFECT OF COLD ROLLING AND ANNEALING ON THE TEXTURE OF Ti-18Nb-4Sn ALLOY. Acta Metall Sin, 2008, 44(11): 1310-1315 .

Download:  PDF(3333KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The microstructures, phase structures and textures of Ti-18Nb-4Sn alloy after cold rolling reduction of 75% and 97% respectively and annealing at 800℃ for different time were measured. It was found that after cold deformation, the sample remained as a single body-centered cubic β phase structure and had rolling texture, and microstructures were characterized by rolling lines. With increasing cold rolling reduction, the intensity of rolling texture changed from weak to strong, At the reduction of 97%, rolling texture were mainly {223} <110> and {112}<110>. After annealing at 800℃ for five minutes, recrystallization was occurred in the samples, and microstructures were made of a large number of equiaxed recrystal grain. After annealing at 800 ℃ for one hour, the recrystallized grain grew. Texture analysis showed that the annealing can not significantly affect the texture of the lower reduction sample, while the texture intensity of the high reduction sample rose sharply after annealing, and a particularly strong annealing texture {111}<112> appeared in the samples. After annealing at 800 ° C for five minutes, the texture state of the high reduction sample was stabilized, and not changed even annealing time extended to one hour.
Key words:       
Received:  02 November 2007     
ZTFLH:  TG146.3  

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y2008/V44/I11/1310

[1]Niinomi M.Metall Mater Trans,2002;33A:477
[2]Kim H Y,Satoru H,Kim J I,Hosoda H,Miyazaki S.Mater Trans,2004;45:2443
[3]Inamura T,Fukui Y,Hosoda H,Wakashima K,Miyazaki S.Mater Trans,2004;45:1083
[4]Laheurte P,Eberhardt A,Philippe M J.Mater Sci Eng, 2005;A396:223
[5]Masumoto K,Horiuchi Y,Inamura T,Hosoda H, Wakashima K,Kim H Y,Miyazaki S.Mater Sci Eng,2006: A438-440:835
[6]Inamura T,Kinoshita Y,Kim J I,Kim H Y,Hosoda H, Wakashima K,Miyazaki S.Mater Sci Eng,2006:A438- 440:865
[7]Kim H S,Lira S H,Yeo I D,Kim W Y.Mater Sci Eng, 2007:A449-451:322
[8]Kim H Y,Sasaki T,Okutsu K,Kim J I,Inamura T, Hosoda H,Miyazaki S.Acta Mater,2006;54:423
[9]Matsumoto H,Watanabe S,Hanada S.J Alloys Compd, 2007;439:146
[10]Bunge J H.Metheden der Texturanalyse.Berlin: Akademie Verlag,1969:20
[11]Ray R K,Jonas J J,Hook R E.Int Mater Rev,1994;39: 129
[12]Matsumoto H,Watanabe S,Hanada S.Mater Trans,2005; 46:1070
[13]Sander B,Raabe D.Mater Sci Eng,2008;A479:236
[1] WANG Luning, LIU Lijun, YAN Yu, YANG Kun, LU Lili. Influences of Protein Adsorption on the in vitro Corrosion of Biomedical Metals[J]. 金属学报, 2021, 57(1): 1-15.
[2] TUNG Feng'en;WANG Yuming Institute of Materials Science; Jilin University; Changchun. X-RAY ANALYSIS OF WORK-HARDENING PROCESS FOR POLYCRYSTALLINE а-BRASS DURING UNIAXIAL TENSILE TEST[J]. 金属学报, 1989, 25(2): 82-84.
[3] WANG Jinliang, WANG Chenchong, HUANG Minghao, HU Jun, XU Wei. The Effects and Mechanisms of Pre-Deformation with Low Strain on Temperature-Induced Martensitic Transformation[J]. 金属学报, 2021, 57(5): 575-585.
[4] DU Hegui;LIU Xin Northeast University of Technology; Shenyang. KINETICS OF CARBON COMBUSTION IN PLASMA AIR[J]. 金属学报, 1989, 25(2): 85-88.
[5] . [J]. 金属学报, 2001, 37(1): 42-46 .
[6] . [J]. 金属学报, 1999, 35(3): 320-324 .
[7] . [J]. 金属学报, 2000, 36(1): 72-76 .
[8] . [J]. 金属学报, 1999, 35(3): 330-333 .
[9] . [J]. 金属学报, 1999, 35(3): 334-336 .
[10] . [J]. 金属学报, 2000, 36(6): 647-650 .
[11] . [J]. 金属学报, 2000, 36(6): 655-658 .
[12] No Author. ACTA METALLURGLCA SLNLCA Volume 28 Series A 1992 SUBJECT INDEX[J]. 金属学报, 1992, 28(12): 63-90.
[13] . [J]. 金属学报, 2000, 36(7): 780-784 .
[14] No Author. ACTA METALLURGICA SINICA(JINSHU XUEBAO) Volume 28 1992 AUTHOR INDEX[J]. 金属学报, 1992, 28(12): 71-94.
[15] Хань Яо-вэнь Инсмцмум мемаддов АН КНР;Г.н.Ойкс Московскц цнсмцмум смадц. НЗУЧЕНИЕ ПРОЦЕССОВ ДЕСУЛЬФУРАЦИИ ХНДКОΓО МЕТАЛЛА В ВАКУУМЕ[J]. 金属学报, 1963, 6(2): 98-110.
No Suggested Reading articles found!