| The very high cycle fatigue properties of bearing steel GCr15 prepared by two processing routes |
| Yongde LI;;shou xin LI;;;; |
| 沈阳中科院金属研究所疲劳部 |
|
Cite this article:
Yongde LI; shou xin LI. The very high cycle fatigue properties of bearing steel GCr15 prepared by two processing routes. Acta Metall Sin, 2008, 44(8): 968-972 .
|
|
|
Abstract Abstract: The very high cycle fatigue properties of bearing steel GCr15 prepared by two processing routes are studied in this paper. It is demonstrated that compared with vacuum melting (VM), the specimens prepared by electroslag remelting (ER) have smaller and narrow distribution of the inclusion size. Therefore, the specimens prepared by ER exhibit a better fatigue property. Experimental results and theoretical analysis demonstrate that the stress intensity factor range at the GBF boundary , ΔKGBF , keeps a constant if the steels are with an identical strength, and it will decrease with the increase of yield strength.
|
|
Received: 14 December 2007
|
|
|
[1]Bathias C.Fatigue Fract Eng Mater Struct,1999;22:559 [2]Wang Q Y,Berard J Y,Dubarre A,Baudry G,Rathery S,Bathias C.Fatigue Fract Eng Mater Struct,1999;22: 667 [3]Murakami Y.Metal Fatigue:Effects of Small Defects and Nonmetallic Inclusions.Amsterdam & Boston:Elsevier, 2002:273 [4]Murakami Y,Nomoto T,Ueda T,Murakami Y.Fatigue Fract Eng Mater Struct,2000;23:893 [5]Murakami Y,Nomoto T,Ueda T,Murakami Y.Fatigue Fract Eng Mater Struct,2000;23:903 [6]Shiozawa K,Lu L,Ishihara S.Fatigue Fract Eng Mater Struct,2001;24:781 [7]Shiozawa K,Morii Y,Nishino S,Lu L.Int J Fatigue,2006; 28:1521 [8]Chapetti M D,Tagawa T,Miyata T.Mater Sci Eng,2003; A356:227 [9]Chapetti M D,Tagawa T,Miyata T.Mater Sci Eng,2003; A356:236 [10]Murakami Y.Metal Fatigue:Effects of Small Defects and Nonmetallic Inclusions.Amsterdam & Boston:Elsevier, 2002:35 [11]Yang Z G,Zhang J M,Li S X,Li G Y,Wang Q Y,Hui W J,Weng Y Q.Mater Sci Eng,2006;A427:167 [12]Zhang J M,Li S X,Yang Z G.,Li G Y,Hui W J,Weng Y Q.Int J Fatigue,2007;29:765 [13]Yang Z G,Zhang J M,Li S X,Li G Y,Wang Q Y,Hui W J,Weng Y Q.Acta Metall Sin,2005;41:1136 (杨振国,张继明,李守新,李广义,王清远,惠卫军,翁宇庆.金属学报,2005;41:1136) [14]Murakami Y.Metal Fatigue:Effects of Small Defects and Nonmetallic Inclusions.Amsterdam & Boston:Elsevier, 2002:17 [15]Sakai T,Sato Y,Oguma N.Fatigue Fract Eng Mater Struct,2002;25:765 [16]Yang Z G,Li S X,Liu Y B,Li Y D,Li G Y,Hui W J, Weng Y Q.Int J Fatigue,2008;30:1016t |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|