| PREPARATION OF LIGHT RADAR ABSORBING MATERIALS WITH BROAD BANDWIDTH BY MIXING IRON NANOFIBERS WITH CARBONYL IRON PARTICLES |
| TONG Guo-Xing |
| 武汉理工大学国家重点实验室 |
|
Cite this article:
TONG Guo-Xing. PREPARATION OF LIGHT RADAR ABSORBING MATERIALS WITH BROAD BANDWIDTH BY MIXING IRON NANOFIBERS WITH CARBONYL IRON PARTICLES. Acta Metall Sin, 2008, 44(8): 1001-1005 .
|
|
|
Abstract In view of the high density and low permittivity of the carbonyl iron particles, the light absorbing coatings with broad bandwidth were fabricated by decreasing the mass fraction of carbonyl iron particles and mixing the iron nanofibers with low density and high permittivity into the absorbent. The influences of the mass fraction of the iron nanofibers on the microwave electromagnetic and absorbing properties of the iron nanofibers/carbonyl iron particles composites were investigated. The results showed that the complex permittivity and permeability of the composites increased with the increase of the mass fraction of the iron nanofibers. The absorbing coatings based on the composites consisting of 2.2-4.4 wt% iron nanofibers exhibited a broader bandwidth and lower surface density than that of the absorbing coatings based on carbonyl iron particles, which was attributed to the enhancing of the matching and absorbing properties of the absorbing coatings through the increase of the complex permittivity of the absorbent in an appropriate range. Thereforre, a new method was provided for the preparation of the light absorbing absorbing coatings with broad bandwidth.
|
|
Received: 23 November 2007
|
|
|
[1]He Y F,Gong R Z,Li X C,Wang X,He H H.J Inorg Mater,2006;21:1449 (何燕飞,龚荣洲,李享成,王鲜,何华辉.无机材料学报,2006;21:1449) [2]Duan Y P,Liu S H,Wen B,Guan H T,Wang G Q.J Compos Mater,2006;40:1841 [3]Petrov V M,Gagulin V V.Inorg Mater,2001;37:93 [4]Tong G X,Wang W,Guan J G,Zhang Q J.J Inorg Mater, 2006;21:1461 (童国秀,王维,官建国,张清杰.无机材料学报,2006;21:1461) [5]Wang W,Guan J G,Wang Q.J Inorg Mater,2005;20: 599 (王维,官建国,王琦.无机材料学报,2005;20:599) [6]Liu J H,Zhou X M,Li S M.Acta Mater Compos Sin, 2005;22:70 (刘建华,周新楣,李松梅.复合材料学报,2005;22:70) [7]Ma R,Bando Y,Sato T.Chem Phys Lett,2001;350:1 [8]Yang Y,Zhang B S,Xu W D,Shi Y B,Zhou N S,Lu H X.J Alloy Compd,2004;365:300 [9]Kuhn L T,Bojesen A,Timmermann L,Nielsen M M, Mφrup S.J Phys:Condens Mater,2002;14:13551 [10]Park M J,Choi J,Kim S S.IEEE Trans Magn,2000;36: 3272 [11]Xie W,Cheng H F,Chu Z Y,Tang G P,Mu W D,Chen Z H.J Funct Mater,2006;37:1201 (谢炜,程海峰,楚增勇,唐耿平,穆武第,陈朝辉.功能材料,2006;37:1201) [12]Gan Z P,Guan J G,Deng H Y,Yuan R Z.Acta Electron Sin.2003;31:918 (甘治平,官建国,邓惠勇,袁润章.电子学报,2003;31:918) |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|