| A Model for Calculating Solubility of Hydrogen in Molten Alloys |
| ;;;; |
| 清华大学机械工程系 |
|
Cite this article:
. A Model for Calculating Solubility of Hydrogen in Molten Alloys. Acta Metall Sin, 2008, 44(2): 129-133 .
|
|
|
Abstract Based on the Sieverts law and the thermodynamic model for activity coefficient
prediction, a new thermodynamic model has been developed for calculating the hydrogen so-
lubility in molten multicomponent alloys in which only the hydrogen solubilities in pure met-
als are required. The predicted hydrogen solubilities in several molten aluminum alloys at
different temperatures and compositions have a good agreement with the experimental results.
|
|
Received: 08 May 2007
|
[1]Lei Y Q.Physical Chemistry in the Cast Processing.Bei- jing:New Times Press,1982:155 (雷永泉.铸造过程物理化学.北京:新时代出版社,1982:155) [2]Translated by Huang L Y,Yah M S.Gases in Nonferrous Metals and Alloys.Beijing:Met- allurgical Industry Press,1989:1,54,126 (著.黄良余,严名山译.有色金属及其合金中的气体.北京:冶金工业出版社,1989:1,54,126) [3]Chen Y D.Hydrogen in Metals and Alloys.Beijing:Met- allurgical Industry Press,1988:12 (陈永定.金属和合金中的氢.北京:冶金工业出版社,1988:12) [4]Xiong Y C,Huang Z G,Wang W Q.Spec Cast Nonferrous Alloys,1995;(4):12 (熊艳才,黄志光,王文清.特种铸造及有色合金,1995;(4):12) [5]Baccepman A M,Kunin A A,Syrovoi I N;Translated by Zhang Z H,Jin Q G.Measurement of the Gas in Metals. Shanghai:Shanghai Science & Technology Press,1981:1 (著.张中豪,金钦漧译.金属中气体的测定.上海:上海科学技术出版社,1981:1) [6]Manchester P D.Phase Diagrams of Binary Hydrogen Al- loys.Materials Park,OH:ASM International,2000:1 [7]Lin R Y,Hoch M.Metall Trans,1989;20A:1785 [8]Anyalebechi P N.Scr Mater,1996;34:513 [9]Anyalebechi P N.Scr Metall Mater,1995;33:1209 [10]Wagner C.Thermodynamics of Alloys. Cambridge: Addison-Wesley Press,1952:120 [11]Sokolov V M,Fedorenko I V.Int J Hydrogen Energy,1996; 11-12:931 [12]Jiang G R,Liu Y,Li Y X,Su Y Q,Guo J J.Acta Metall Sin,2007;43:503 (蒋光锐,刘源,李言祥,苏彦庆,郭景杰.金属学报,2007;43:503) [13]Li M.Master Thesis,Harbin Institute of Technology,2006 (李敏.哈尔滨工业大学硕士学位论文,2006) [14]Anyalebechi P N,Talbot D E J,Granger D A.Metall Trans,1988;19B:227 [15]Xu Z Y,Li L.Materials Thermodynamic.Beijing:Science Press,2005:265 (徐祖耀,李麟.材料热力学.北京:科学出版社,2005:265) [16]Kung J K,Nazarlo F N,Joffe J,Tassios D.Ind Eng Chem Process Des Dev,1984;23:170 [17]Ding X Y,Wang W Z.Acta Metall Sin,1994;30:444 (丁学勇,王文忠.金属学报,1994;30:444) [18]Gokcen N A.Statistical Thermodynamics of Alloys.New York:Plenum Press,1986:255 [19]Takamichi I,G.Roderick I L.The Physical Properties of Liquid Metals.New York:Oxford University Press,1988: 6 [20]Tao D P.Metall Mater Trans,2005;36A:3495 [21]Zhang H W,Li Y X,Liu Y.Acta Metall Sin,2007;43: 113 (张华伟,李言祥,刘源.金属学报,2007;43:113) [22]Matysina Z A,Zaginaichenko S Y,Schur D V,Pishuk V K.J Alloy Compd,2002;330-332:85 [23]Mao Y W.Metallurgical Melts.Beijing:Metallurgical In- dustry Press,1993:1 (毛裕文.冶金熔体.北京:冶金工业出版社,1993:1)r |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|