| Low-temperature nanocrystallization of FeSiB amorphous alloys produced by low-frequency magnetic pulsing |
| CHAO Yuesheng; ZHANG Yanhui; GUO Hong; ZHANG LI; WANG Xinggang |
| College of Science; Northeastern University; Shenyang 110004 |
|
Cite this article:
CHAO Yuesheng; ZHANG Yanhui; GUO Hong; ZHANG LI; WANG Xinggang. Low-temperature nanocrystallization of FeSiB amorphous alloys produced by low-frequency magnetic pulsing. Acta Metall Sin, 2007, 43(3): 231-234 .
[1]Lu K,Zhou F.Acta Metall Sin,1997;33:99 (卢柯,周飞.金属学报,1997;33:99) [2]Wu W F,Yao K F.Rere Met Mater Eng,2005;34:505 (吴文飞,姚可夫.稀有金属材料与工程,2005;34:505) [3]Kulik T,Horubata T,Matyja H.Mater Sci Eng,1992; A157:107 [4]Qi M,Wang Y,Wang Y N,Yang D Z.J Funct Mater, 2005;36(1):35 (齐民,王岩,王轶农,扬大智.功能材料,2005;36(1): 35) [5]Yoshizawa Y,Oguma S,Yamauchi K.J Appl Phys,1988; 64:6044 [6]Long Y,Zhang Z Y,Li S W.Functional Magnetic Mate- rials and Its Applications.Beijing:China Machine Press, ??1997:115 (龙毅,张正义,李守卫.功能磁性材料及其应用.北京:机械工业出版社,1997:115) [7]Tong H Y,Wang J T,Ding B Z,Jiang H G,Lu K.J Non-Cryst Solids,1992;150:444 [8]Vazquez M,Marin P,Leccabue F,Watts B E,Deriu A, Negri D,Bocelli G.IEEE Trans Magn,1993;29:2685 [9]Chao Y S,Li M Y,Geng Y,Liu J G.Acta Phys Sin,2004; 53:3453 (晁月盛,李明扬,耿岩,刘吉刚.物理学报,2004;53:3453) [10]Rbulsala A,Gammaitoni L.Phys Today,1996:39 [11]Shao Y Z,Zhong W R,Lin G M,Li J C.Acta Phys Sin, 2004;53:3157 (邵元智,钟伟荣,林光明,李坚灿.物理学报,2004;53:3157) [12]Gibb T C.Principles of M(?)ssbauer Spectroscopy.London: Chapman and Hall,1976:41 [13]Guo Y C,Wang Z X.The Physics of Noncrystal State. Beijing:Science Press,1984:175 (郭贻诚,王震西.非晶态物理学.北京:科学出版社,1984: 175) [14]Tong H Y,Ding B Z,Wang J T,Lu K.J Appl Phys,1992; 72:5124 [15]Lai Z H,Conrad H,Chao Y S,Wang S Q,Sun J.Scr Metall,1989;23:305 [16]Lai Z H,Conrad H,Teng G Q,Chao Y S.Mater Sci Eng, 2000;A287:238 [17]Xiao S H,Chao Y S,Zhou B L.Acta Phys Sin,2000;49: 288 (肖素红,晁月盛,周本廉.物理学报,2000;49:288) |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|