Abstract Al-based stable quasicrystals exist only in ternary alloy systems. According to the cluster line rule, these quasicrystals require three constituent elements. For the objective of determining if there is any quaternary quasicrystal, in this paper we have used the electron concentration and atomic size constant criteria to analyze the alloy phase evolution in the Al-Cu-Ni-Fe quaternary system. We have found no evidence of any quaternary quasicrystal. This result confirms the conclusions out of the cluster line rule that only three elements are sufficient to form a stable Al-based quasicrystal.
|
|
Received: 30 October 2006
|
|
|
[1]Shechtman D,Blech I,Gratias D,Cahn J W.Phys Lett, 1984;53:1951 [2]Dong C.Quasicrystalline Materials.Beijing:National Defence Industry Press,1998:29 (董闯.准晶材料.北京:国防工业出版社,1998:29) [3]Wang R H.Physics in Quasicrystals.Beijing:Science ??Press,2004:4,12 (王仁卉.准晶物理学.北京:科学出版社,2004:4,12) [4]Qiang J B,Wang D H,Bao C M,Wang Y M,Xu W P, Song M L,Dong C.J Mater Res,2001;16:2653 [5]Dong C,Qiang J B,Wang Y M.Philos Mag,2006;86: 263 [6]Mayou D,Cyroy-Lackmann F,de Trambley G,Klein T. J Non-Cryst Solids,1993;153-154:412 [7]Gratias D,Calvayrac Y,Devaud-Rzepski J,Faudot F, Harmelin M,Quivy A,Bancet P A.Non-Cryst Solids, 1993;153-154:482 [8]Dong C,Perrot A,Dubois J M,Belin E.Mater Sci Forum, 1994;150-151:403 [9]Dong C.Chin J Mater Res,1995;9:89 [10]Pearson W B.The Crystal Chemistry and Physics of Met- als and Alloys.New York:Wiley-Interscience,1972:155 [11]Qiang J B,Wang D H,Bao C M.J Mater Res,2001;16: 2653 [12]Tsuda K,Terauchi M,Fujiwara A,Tsai A P.Inoue A, Masumoto T.J Non-Cryst Solids,1993:153:98 [13]Niessen A K,de Boer F R,Boom R,de Chatel P F,Mat- tens W C M,Miedema A R.CALPHAD,1983;7:51 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|