| Softening Mechanism of Boron—Bearing Low--Carbon Hot Strips Produced by TSCR Route |
| QIU Shengtao; XIAO Lijun; LIU Jiaqi; GAN Yong |
| State Key Laboratory of Advanced Steel Processes and Products; Central Iron and Steel Research Institute; Beijing 100081 |
|
Cite this article:
QIU Shengtao; XIAO Lijun; LIU Jiaqi; GAN Yong. Softening Mechanism of Boron—Bearing Low--Carbon Hot Strips Produced by TSCR Route. Acta Metall Sin, 2006, 42(11): 1202-1206 .
|
|
|
Abstract The SPHC (Steel Plate Heat Commercial) hot strips containing 10ppm~50ppm B were produced in the simulation of TSCR production route in the laboratory,the effects of boron micro-alloying on the microstucture,precipitates and mechanical properties were investigated.The results showed that the grain-size scale of the SPHC hot strips containing 10ppm~50ppm B can attain to 7~8 grade,the mean grain size was up to 22~35μm, the yield strength decreased by 94Mpa.
|
|
Received: 24 February 2006
|
|
|
[1] Takahashi N, Shibata M. Conf Proc on Technology of Continuous Annealed Cold-Rolled Sheet Steel, Warren-dale, PA: TMS-AIME, 1984: 133 [2] Sudo M, Tsukatani I. Conf Proc on Technology of Continuous Annealed Cold-Rolled Sheet Steel. Warrendale, PA: TMS-AIME, 1984: 203 [3] Kang Y L, Yu H. Sci Technol Eng, 2005; 5(5): 305 (康永林,于浩.科学技术与工程, 2005;5(5):305) [4] Gao N, Baker T N. ISIJ Int, 1998; 38; 7: 744 [5] Manohar P A. ISIJ Int, 1998; 38: 799 [6] Miyahara M, Nakajima N, Kuramoto K. R&D Kobe Steel Enpinering Rep, 1990; 36(3): 61 (宫原征行,中岛悟博,藏本腾次郎,R.D神户制钢技报,1990; 36(3):61) [7] Choquet P, Febregue P, Giusti J, Chamont B, Pezant J N. Int Symp on Mathematical Modeling of Hot Rolling of Steel, Canada, 1990; 33 [8] Yong Q L, Sun X J, Liu Q Y, Zhang C, Li J K. Spec Steel, 2005; 26(1): 1 (雍岐龙,孙新军,刘清友,张晨,李继康.特殊钢,2005; 26(1):1) [9] Cahn R W, Haasen P, Kramer E J. Translated by Liu J H et al. Materials Science and Technology. Vol.7, Beijing: Science Press, 1999: 97 (Cahn R W,Haasen P,Kramer E J.刘嘉禾等译.材料科学与技术丛书.第7卷,北京:科学出版社,1999:97) |