In Situ Observation of Relativity between Domain and Indentation Crack Propagating in Barium Titanate Single Crystal
天津科技大学
Cite this article: 

. In Situ Observation of Relativity between Domain and Indentation Crack Propagating in Barium Titanate Single Crystal. Acta Metall Sin, 2006, 42(12): 1274-1278 .

Download:  PDF(1957KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  Instant electric field-induced 90 domain switching, crack initiation and propagation in a poled BaTiO3 single crystal, as well as sustained field-induced indentation crack propagation and 90 domain switching in an unpoled BaTiO3 single crystal have been investigated in situ using optical microscopy. The results show that 90 domain switching is a prerequisite for instant field-induced crack initiation and propagation, but that is no direct relation between the site of crack initiation and propagation and the domain switching zones. Delayed propagation of unloaded indentation crack under sustained field can result in enlargement of the indent ation-induced 90 domain switching zones.
Key words:       
Received:  14 March 2006     
ZTFLH:  TG113.2  
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y2006/V42/I12/1274

[1] Yang W, Fang F, Tao M. Int J Solids Struct, 2001; 38: 2203
[2] Busche M J, Hsia K J. Scr Mater, 2001; 44: 207
[3] Fang F, Yang W. Mater Lett, 2002; 57: 198
[4] Li F X, Li S, Fang D N. Mater Sci Eng, 2005, B120: 119
[5] Zhao X W, Chu W Y, Su Y J, Li J X, Gao K W, Qiao L J. Acta. Metall Sin, 2006; 42: 13 (赵显武,褚武扬,宿彦京,李金许,高克玮,乔利杰.金属学报,2006;42:13)
[6] Chung H T, Shin B C, Kim H G. J Am Ceram Soc, 1989; 72: 327
[7] Wang Y, Chu W Y, Gao K W, Su Y J, Qiao L J. Appl Phys Lett, 2003; 82: 1583
[8] Chantikul P, Anstis G R, Laun B R, Marshall D B. J Am Ceram Soc, 1981; 64: 539
[9] Fang F, Yang W. Mater Lett, 2000; 46: 131
[10] Zhu T, Yang W. Mech Phys Solids, 1999; 47: 81
[11] Zhang T Y, Wang T H, Zhao M H. Acta Mater, 2003; 51: 4881
[12] Wang R M, Chu W Y, Gao K W, Su Y J, Qiao L J. Mater Lett, 2004; 58: 1811
[1] WANG Luning, LIU Lijun, YAN Yu, YANG Kun, LU Lili. Influences of Protein Adsorption on the in vitro Corrosion of Biomedical Metals[J]. 金属学报, 2021, 57(1): 1-15.
[2] TUNG Feng'en;WANG Yuming Institute of Materials Science; Jilin University; Changchun. X-RAY ANALYSIS OF WORK-HARDENING PROCESS FOR POLYCRYSTALLINE а-BRASS DURING UNIAXIAL TENSILE TEST[J]. 金属学报, 1989, 25(2): 82-84.
[3] WANG Jinliang, WANG Chenchong, HUANG Minghao, HU Jun, XU Wei. The Effects and Mechanisms of Pre-Deformation with Low Strain on Temperature-Induced Martensitic Transformation[J]. 金属学报, 2021, 57(5): 575-585.
[4] DU Hegui;LIU Xin Northeast University of Technology; Shenyang. KINETICS OF CARBON COMBUSTION IN PLASMA AIR[J]. 金属学报, 1989, 25(2): 85-88.
[5] . [J]. 金属学报, 2001, 37(1): 42-46 .
[6] . [J]. 金属学报, 1999, 35(3): 320-324 .
[7] . [J]. 金属学报, 2000, 36(1): 72-76 .
[8] . [J]. 金属学报, 1999, 35(3): 330-333 .
[9] . [J]. 金属学报, 1999, 35(3): 334-336 .
[10] . [J]. 金属学报, 2000, 36(6): 647-650 .
[11] . [J]. 金属学报, 2000, 36(6): 655-658 .
[12] No Author. ACTA METALLURGLCA SLNLCA Volume 28 Series A 1992 SUBJECT INDEX[J]. 金属学报, 1992, 28(12): 63-90.
[13] . [J]. 金属学报, 2000, 36(7): 780-784 .
[14] No Author. ACTA METALLURGICA SINICA(JINSHU XUEBAO) Volume 28 1992 AUTHOR INDEX[J]. 金属学报, 1992, 28(12): 71-94.
[15] Хань Яо-вэнь Инсмцмум мемаддов АН КНР;Г.н.Ойкс Московскц цнсмцмум смадц. НЗУЧЕНИЕ ПРОЦЕССОВ ДЕСУЛЬФУРАЦИИ ХНДКОΓО МЕТАЛЛА В ВАКУУМЕ[J]. 金属学报, 1963, 6(2): 98-110.
No Suggested Reading articles found!