NEW METHOD FOR PREDICTION OF JOMINY CURVE OF STRUCTURAL STEEL
吉林大学材料学院
Cite this article: 

. NEW METHOD FOR PREDICTION OF JOMINY CURVE OF STRUCTURAL STEEL. Acta Metall Sin, 2006, 42(4): 405-410 .

Download:  PDF(705KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  This paper presents a novel method for predicting the Jominy curve of structural steels. An analytical function containing the undetermined parameter was used to calculate the Jominy hardness distributions. This undetermined parameter was defined as the hardenability coefficient of steel, which is different from the conventional element coefficient and depends on the descending velocity of the Jominy curve. Therefore, the problem predicting the Jominy curve changes to one calculating the hardenability coefficient. It was demonstrated that the hardenability coefficient depends on the chemical composition under the condition of the standard Jominy test. An empirical relationship between the hardenability coefficient and the chemical composition of structural steels has been established using a subsection approach. Substituting the obtained hardenability coefficient into the distribution model of the hardness, the predicted Jominy curves exhibited very good agreements with the experimental data.
Key words:  Jominy curve      hardenability coefficient      chemical composition      
Received:  10 November 2005     
ZTFLH:  TG115.6  
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y2006/V42/I4/405

[1] Field J. Met Prog, 1943; 143: 402
[2] Grossmann M A. Trans AIME, 1942; 154: 227
[3] Deretana A F, Doane D V. Met Prog, 1971; 100: 65
[4] Jatczak C F. Metall Trans, 1973; 4: 2272
[5] Coates D F. Metall Trans, 1973; 4: 2313
[6] Sharma B C, Purdy G R. Metall Trans, 1973; 4: 2303
[7] Sponzilli J T, Keith C J, Walter G H. Met Prog, 1975; 108: 86
[8] Sponzilli J T, Walter G H, Breen D H. Met Eng Q, 1976; 16: 57
[9] Tartaglia J M, Eldis G T. Metall Trans, 1984; 15A: 1173
[10] Thomas K, Gearv E A, Avis P, Bishop D. Mater Design, 1992; 13: 17
[11] Mostert R J, van Rooyen G T. Mater Sci Technol, 1991; 7: 803
[12] Li M V, Niebuhr D V, Meekisho L L, Atteridge D G. Met- all Mater Trans, 1998; 29B: 661
[13] Dobrzanski L A, Sitek W. J Mater Process Technol, 1997; 64: 117
[14] Just E. Met Prog, 1969; 95: 871
[15] Breen D H, Walter G H, Sponzilli J T. Met Prog, 1973; 104: 43
[16] Yu B H. Iron Steel, 1985; 20(3): 40 (余柏海.钢铁,1985;20(3):40)
[17] Lund T. Scandi J Metall, 1990; 19: 227
[18] Andersson K, Kivivuori S, Korhonen A S. Mater Sci Forum, 1994; 163: 683
[19] Filetin T, Liscic B, Galinec J. Adv Mater Proc, 1995; 148: 2
[20] Cook W T, Morris P F, Woollard L. J Mater Eng Perform, 1997; 6: 443
[21] Komenda J, Sandstrom R, Thkiainen M. Steel Res, 1997; 89: 132
[22] Dobrzanski L A, Sitik W. J Mater Process Technol, 1999; 90: 467
[23] Miu Z H, Hu W Y. Trans Met Heat Treat, 2000; 21(1): 57 (缪宗华,胡为颖.金属热处理学报, 2000;21(1):57)
[24] Jin M, Lian J S, Jing Z H. Acta Metall Sin, 2006; 42: 265 (金 满,连建设,江中浩.金属学报, 2006;42:265)
[25] AMS Handbook Committee. Metals Handbook. 9th ed., Vol.1, Ohio, USA: American Society for Metals, 1978
[26] Wu J X, Zhou G Y, Xun Y M. Application and Technology of Hardenability of Steels. Beijing: China Machine Press, 1994: 139 (吴季恂,周光裕,苟毓闽.钢的淬透性应用技术.北京:机械 工业出版社,1994:139)
[27] Fu D Z, Lin H G. Hardenability Handbook of Steels. Beijing: China Machine Press, 1973: 88 (傅代直,林慧国.钢的淬透性手册.北京:机械工业出版社, 1973:88)
[28] Heattreatment Handbook Edit Committee, Heattreatment Handbook. Vol.4, Beijing: China Machine Press, 1992: 558 (热处理手册编辑委员会.热处理手册.第4卷,北京:机械工 业出版社,1992:558)
[1] ZHANG Beijiang,HUANG Shuo,ZHANG Wenyun,TIAN Qiang,CHEN Shifu. Recent Development of Nickel-Based Disc Alloys andCorresponding Cast-Wrought Processing Techniques[J]. 金属学报, 2019, 55(9): 1095-1114.
[2] Shujun CHEN, Xuan WANG, Tao YUAN, Xiaoxu LI. Research on Prediction Method of Liquation Cracking Susceptibility to Magnesium Alloy Welds[J]. 金属学报, 2018, 54(12): 1735-1744.
[3] Kaiwen WEI,Zemin WANG,Xiaoyan ZENG. ELEMENT LOSS OF AZ91D MAGNESIUM ALLOY DURING SELECTIVE LASER MELTING PROCESS[J]. 金属学报, 2016, 52(2): 184-190.
[4] DING Jie, ZHANG Zhiming, WANG Jianqiu, HAN En-Hou, TANG Weibao, ZHANG Maolong, SUN Zhiyuan. MICRO-CHARACTERIZATION OF DISSIMILAR METAL WELD JOINT FOR CONNECTING PIPE- NOZZLE TO SAFE-END IN GENERATION III NUCLEAR POWER PLANT[J]. 金属学报, 2015, 51(4): 425-439.
[5] . A NEW MATHEMATICAL MODEL FOR HARDENABILITY OF STEELS[J]. 金属学报, 2006, 42(3): 265-272 .
[6] . MATHEMATICAL MODEL OF U-CURVE OF STEELS[J]. 金属学报, 2006, 42(10): 1019-1024 .
No Suggested Reading articles found!