Enhanced plasticity of bulk metallic glass composite containing as-cast in situ formed ductile phase dendrite dispersions
南京理工大学金属纳米材料与技术联合实验室
Cite this article: 

. Enhanced plasticity of bulk metallic glass composite containing as-cast in situ formed ductile phase dendrite dispersions. Acta Metall Sin, 2006, 42(3): 331-336 .

Download:  PDF(438KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  An as-cast in situ Zr56.2Ti13.8Nb5.0Cu6.9Ni5.6Be12.5 bulk metallic glass composite with enhanced plasticity was prepared by water quenching, which contains a ductile bcc β-Zr solid solution. The β phase with a volume fraction of about 30% possesses a developed dendritic morphology. The present composite exhibits a pure plastic strain of 10.2% combined with a large elastic strain limit of 2% and a high ultimate strength of 1778MPa upon room-temperature compression. Microscopic observation shows numbers of wavelike shear bands dispersed on the surface of deformed compressive samples
Key words:  water quenching      as-cast in situ formed ductile dendritic crystalline phase      bulk metallic glass comp     
Received:  29 April 2005     
ZTFLH:  TB331  
  TG113.25  
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y2006/V42/I3/331

[1] Zhang T, Inoue A, Masumoto T. Mater Trans JIM, 1991; 32: 1005
[2] Peker A, Johnson W L. Appl Phys Lett, 1993; 63: 2342
[3] Eckert J, He G, Das J, Loser W. Mater Trans, 2003; 44: 1999
[4] Choi-Yim H, Johnson W L. Appl Phys Lett, 1997; 71: 3808
[5] Conner R D, Dandliker R B, Johnson W L. Acta Mater, 1998; 46: 6089
[6] Fan C, Li C F, Inoue A. Phys Rev, 2000; 61B: R3761
[7] Hays C C, Kim C P, Johnson W L. Phys Rev Lett, 2000; 84: 2901
[8] Szuecs F, Kim C P, Johnson W L. Acta Mater, 2001; 49: 1507
[9] Kim C P. PhD Thesis, California Institute of Technology, Pasadena, California, 2001
[10] Hufnagel T C, Fan C, Ott T R, Li J, Brennan S. Inter- metallics, 2002; 10: 1163
[11] Eckert J, Kuhn U, Mattern N, He G, Gebert A. Inter- metallics, 2002; 10: 1183
[12] Lee M H, Lee J Y, Bae D H, Kim W T, Sordelet D S, Kim D H. Intermetallics, 2004; 12: 1133
[13] He G, Eckert J, Loser W, Schultz L. Nature Mater, 2003; 2: 33
[14] Das J, Loser W, Kiihn U, Eckert J, Roy S K, Schultz L. Appl Phys Lett, 2003; 82: 4690
[15] He G, Zhang Z F, Loser W, Eckert J, Schultz L. Ada Mater, 2003; 51: 2383
[1] Yanchun ZHAO, Hao SUN, Chunling LI, Jianlong JIANG, Ruipeng MAO, Shengzhong KOU, Chunyan LI. High Temperature Deformation Behavior of High Strength and Toughness Ti-Ni Base Bulk Metallic Glass Composites[J]. 金属学报, 2018, 54(12): 1818-1824.
[2] LI Jiguang DING Yajie PENG Xingdong LIU Jinwei. EFFECTS OF WATER QUENCHING PROCESS ON THE MICROSTRUCTURE AND MECHANICAL PROPERTIES OF TWIP STEEL[J]. 金属学报, 2010, 46(2): 221-226.
No Suggested Reading articles found!