| SURFACE MODIFICATION OF DIE CASTING Al ALLOY ADC12 WITH HIGH Si CONTENT BY MICRO-ARC OXIDIZATION |
| ZHANG Yongjun; LI Wenfang;WANG Fuhui |
| Institute of Materials Science and echnology; College of Mechanical Engineering; South China University of Technology; Guangzhou 510640 |
|
Cite this article:
ZHANG Yongjun; LI Wenfang; WANG Fuhui. SURFACE MODIFICATION OF DIE CASTING Al ALLOY ADC12 WITH HIGH Si CONTENT BY MICRO-ARC OXIDIZATION. Acta Metall Sin, 2005, 41(12): 1289-1292 .
|
|
|
Abstract Ceramic coating on the surface of die casting Al alloy ADC12 with high Si
content has been prepared by micro-arc oxidization (MAO) in an
electrolyte containing Na2SiO3 and Na3PO4 as its major
compositions at constant current density. The testing results of hardness
and corrosion protection indicate that the obtained ceramic coating has
relatively high microhardness (HV up to 1430) and could provide
effective protection to substrate. Eddy currency thickness measurement
and SEM micrographs manifest that the ceramic coating consists of a
double-layer structure and its thickness is relatively even. EDX and
XRD analyses reveal that the main elements in the coating are O, Al, Si
as well as P, and that the main phases are γ-Al2O3, α-Al2O3. In addition small amounts of
χ-Al2O3, θ-Al2O3 and Al2SiO5 are also detected.
|
|
Received: 06 April 2005
|
|
|
[1] Yerokhin A L, Nie X, Leyland A, Matthews A, Dowey S J. Surf Coat Technol, 1999; 122: 73 [2] Luo S L, Zhou H H, Chen J H, Kuang Y F. Trans Non-ferrous Met Soc Chin, 2002; 12: 491 (罗胜联,周海晖,陈金华,旷亚非.中国有色金属学报,2002; 12:491) [3] Nykyforchyn H M, Klapkiv M D, Posuvailo V M. Surf Coat Technol, 1998; 100-101: 219 [4] Zhang Y J, Yan C W, Wang F H, Lou H Y, Cao C N. Surf Coat Technol, 2002; 161: 36 [5] Zozulin A J, Bartak D E. Met Finish, 1994; 92: 39 [6] Van T B, Brown S D, Wirtz G P. Ceram Bull, 1997; 56: 563 [7] Khaselev O, Weiss D, Yahalom J. Corros Sci, 2001; 43: 1295 [8] Deng Z W, Lai Y C, Xue W B, Chen R Y, Song H W. Nucl Phys Rev, 1997; 14: 193 (邓志威,来永春,薛文彬,陈如意,宋红卫.原子核物理评论, 1997;14:193) [9] McPherson R J. Mater Sci, 1973; 8: 851m |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|