| EXPERIMENTAL RESEARCH ON SULPHUR CONCENTRATION CELL WITH MgS+1.5%ZrS2 SOLID ELECTROLYTE |
| YU Jingkun; LIU Tao; CHEN Min |
| School of Materials & Metallurgy; Northeastern University; Shenyang 110004 |
|
Cite this article:
YU Jingkun; LIU Tao; CHEN Min. EXPERIMENTAL RESEARCH ON SULPHUR CONCENTRATION CELL WITH MgS+1.5%ZrS2 SOLID ELECTROLYTE. Acta Metall Sin, 2005, 41(12): 1285-1288 .
|
|
|
Abstract Large amount of sulphides were synthesized safely by a temperature
gradient method using metals and sublimed sulfur as the raw materials,
and a sulphur concentration cell was developed by using
MgS+1.5%ZrS2 as solid electrolyte and Mo+MoS2 as reference electrode. The sulphur content in carbon--saturated liquid
iron (oxygen activity degreea[O] ≤2×10 -6) at
1623 K was determined by using the prepared sulphur concentration cell.
The gas leakage and splitting crack were solved by optimizing the
structure of solid electrolyte tubes, hydration and oxidation of
the sulphide were also avoided by using special processes. The
results showed that the sulphur concentration cell could be
continuously used with stable signals and good reproducibility.
|
|
Received: 30 March 2005
|
|
|
[1] Taniguchi M, Wakihara M, Uchida T, Hirakawa K, Nii J. Electrochem Soc, 1988; 135: 217 [2] Egaini A, Onoye T, Narita K. Solid State Ionics, 1980; 3/4: 617 [3] Ono K, Moriyama J. Solid State Ionics, 1981; 2: 127 [4] Hong Y R, Jin C J, Li L S, Sun J L. Sens Actuators, 2002; 87B:13 [5] Liu Q G, Worrell W L. Solid State Ionics, 1988; 28-30: 1668 [6] Gozzi D, Granati P. Metall Mater Trans, 1994; 25B: 561 [7] Zhang Z W, Feng G S, Zhang J L, Cao C G. Iron Steel, 2000; 35: 57 (张宗旺,冯根生,张建良,曹传根.钢 铁, 2000;35:57) [8] Gu L J, Tang Z H. Iron Steel, 1984; 19: 13 (古隆建,唐仲和.钢铁, 1984;19:13) [9] Han H O, Wang S L. Solid State Ionics, 1992; 51: 157 [10] Wang S L, Han H O. Steelmaking, 1989; 5: 47 (王舒黎,韩海鸥.炼钢, 1989;5:47) [11] Wang S L, Mao J. Northeast Univ Technol, 1991; 12: 221 (王舒黎,毛杰.东北工学院学报, 1991;12:221) [12] Liu T, Yu J K, Yuan Y H. Northeast Univ (Nat Sci), 2005; 26: 260 (刘涛,于景坤,袁宇皓.东北大学学报(自然科学版),2005; [13] Liu T, Yu J K, Chen M. Northeast Umv (Nat Sci), 2005; 26: 370 26:260) (刘涛,于景坤,陈敏.东北大学学报(自然科学版),2005; 26:370). |
| No Suggested Reading articles found! |
|
|