Acta Metall Sin  2001, Vol. 37 Issue (1): 13-18     DOI:
Research Articles Current Issue | Archive | Adv Search |
Cite this article: 

. . Acta Metall Sin, 2001, 37(1): 13-18 .

Download:  PDF(223KB) 
Export:  BibTeX | EndNote (RIS)      
Key words:       
Received:  10 July 2000     
ZTFLH:  TG132.3  
  TG113.12  
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y2001/V37/I1/13

[1] Kattamis T Z, Flemings M C. TMS-AIME, 1966; 236:1523
[2] Powell G L F, Hogan L M. TMS-AIME, 1969; 245: 407
[3] Walker J L. In: Pierre G R St ed., The Physical Chemistryof Process Metallurgy, Part 2, New York: Interscience,1959: 845
[4] Herlach D M. Mater Sci Eng, 1994; 12R: 177
[5] Schwarz M, Karma A, Eckler K, Herlach D M. Phys RevLett, 1994; 73: 380
[6] Horvay G. J Heat Mass Transfer, 1965; 8: 195
[7] Glicksman M E. Acta Metall, 1965; 13: 1231
[8] Jackson K A, Hunt J D, Uhlmann D R, Seward T P III.TMS-AIDE, 1966; 236: 149
[9] Gartner R F, Norman A F, Greer A L, Zambon A, Ramous E. Acta Mater 1997; 45: 51
[10] Cochrane R F, Herlach D M, Feuerbacher B. Mater SciEng, 1991; 133A: 706
[11] Du W. Ph.D Thesis, Northwestern Polytechnical Universityl Xi'an, 1998(杜 伟。西北工业大学博士学位论文,西安,1998)
[12] Liu F, Cai Y, Guo X F, Yang G C. Casting, 2000; 6: 344
[13] Chakravorty S, West D R F. J Mater Sci, 1984; 19: 3574
[14] Machlin E S, Shao J. Metall Trans, 1978; 9A: 561
[15] Liu F, Guo X F, Cai Y, Yang G C. Acta Metall Sin, 2000;36:567(刘峰,郭学峰,蔡瑜,杨根仓.金属学报,2000;36:567)
[16] Li J F, Yang G C, Zhou Y H. J Cryst Growth,1998; 192:462
[17] Piccone T J, Wu Y, Shiohara Y, Flemings M C. MetallTrans, 1987; 18A: 915
[18] Boettinger W J, Coriell S R, Trivedi R. In: Mehrabian R,Parrish P A eds., Rapid Solidification Processing: Principles and Technologies IV, Baton Rouge, LA, Claitor's,1988: 13
[19] Guo X F. Ph D Thesis, Northwestern Polytechnical Universityl Xi'an, 1999(郭学峰.西北工业大学博士学位论文,西安,1999)
[20] Dahle A K, Thevik H J, Arnberg L, John D H St. MetallMater Trans, 1999; 30B: 287
[1] WANG Luning, LIU Lijun, YAN Yu, YANG Kun, LU Lili. Influences of Protein Adsorption on the in vitro Corrosion of Biomedical Metals[J]. 金属学报, 2021, 57(1): 1-15.
[2] TUNG Feng'en;WANG Yuming Institute of Materials Science; Jilin University; Changchun. X-RAY ANALYSIS OF WORK-HARDENING PROCESS FOR POLYCRYSTALLINE а-BRASS DURING UNIAXIAL TENSILE TEST[J]. 金属学报, 1989, 25(2): 82-84.
[3] WANG Jinliang, WANG Chenchong, HUANG Minghao, HU Jun, XU Wei. The Effects and Mechanisms of Pre-Deformation with Low Strain on Temperature-Induced Martensitic Transformation[J]. 金属学报, 2021, 57(5): 575-585.
[4] DU Hegui;LIU Xin Northeast University of Technology; Shenyang. KINETICS OF CARBON COMBUSTION IN PLASMA AIR[J]. 金属学报, 1989, 25(2): 85-88.
[5] . [J]. 金属学报, 2001, 37(1): 42-46 .
[6] . [J]. 金属学报, 1999, 35(3): 320-324 .
[7] . [J]. 金属学报, 2000, 36(1): 72-76 .
[8] . [J]. 金属学报, 1999, 35(3): 330-333 .
[9] . [J]. 金属学报, 1999, 35(3): 334-336 .
[10] . [J]. 金属学报, 2000, 36(6): 647-650 .
[11] . [J]. 金属学报, 2000, 36(6): 655-658 .
[12] No Author. ACTA METALLURGLCA SLNLCA Volume 28 Series A 1992 SUBJECT INDEX[J]. 金属学报, 1992, 28(12): 63-90.
[13] . [J]. 金属学报, 2000, 36(7): 780-784 .
[14] No Author. ACTA METALLURGICA SINICA(JINSHU XUEBAO) Volume 28 1992 AUTHOR INDEX[J]. 金属学报, 1992, 28(12): 71-94.
[15] Хань Яо-вэнь Инсмцмум мемаддов АН КНР;Г.н.Ойкс Московскц цнсмцмум смадц. НЗУЧЕНИЕ ПРОЦЕССОВ ДЕСУЛЬФУРАЦИИ ХНДКОΓО МЕТАЛЛА В ВАКУУМЕ[J]. 金属学报, 1963, 6(2): 98-110.
No Suggested Reading articles found!