The Structure, Properties and Thermal Stability of the Nanocrystalline Fe-Ti-N Soft Magnetic Films
LI Dan; GU Yousong; CHANG Xiangrong; LI Fushen; QIAO Lijie; TIAN Zhongzhuo; FANG Guangdan; SONG Qingshan
Department of Materials Physics; University of Science & Technology Beijing; Beijing 100083
Cite this article: 

LI Dan; GU Yousong; CHANG Xiangrong; LI Fushen; QIAO Lijie; TIAN Zhongzhuo; FANG Guangdan; SONG Qingshan. The Structure, Properties and Thermal Stability of the Nanocrystalline Fe-Ti-N Soft Magnetic Films. Acta Metall Sin, 2003, 39(2): 204-208 .

Download:  PDF(197KB) 
Export:  BibTeX | EndNote (RIS)      
Key words:       
Received:  22 April 2002     
ZTFLH:  TG113.22  

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y2003/V39/I2/204

[1] Kim T K, Takahashi M. Appl Phys Lett, 1972; 20: 492
[2] Komuro M, Kozono Y, Hanazono M, Sugita Y. J ApplPhys, 1990; 67: 5126
[3] Sugita. Y, Lakaha,shi H, Komuro M, Mitsuoka K, SakumaA. J Appl Phys, 1994; 76: 6687
[4] Sugita. Y, Takahashi 14, Komuro M. Igarashi M, Inmra H, Kambe T. Appl Phys, 1996; 79: 5576
[5] Cadogan ,T M, Aus1 J. Phys, 1997; 50: 1093
[6] Metzger R M, Bao X H, Carbuciccchio M. J Appl Phys,1994; 76: 6626
[7] Coey J M D. J Appl Phys, 1994; 76: 6632
[8] Ishida S, Kitawatase K. J Magn Magn Mater, 1992; 104-107: 1933
[9] Tshida S, Kitawatase K, Fujii S, Asano S. J Phys, 1992; 4:765
[10] Nakajima K, Okamoto S. Appl Phys Lett. 1990; 56: 92
[11] Morisako A, Matsumoto M. Maoe M. J Appl Phys, 1991;69: 5619
[12] Jiang H, Wu Q L, Tao K, Li H D. J Appl Phys. 1995; 78:3299
[13] Yoshitake T, Ohkoshi M. IEEE Trans Magn, 1995; 31:3850
[14] Zhou J P, Li D, Gu Y S, Chang X R, Zhao C H, Li F S,Qiao I J, Tian Z Z, Fang G D, Song Q S. IEEE TransMagn, 2001; 37: 3844
[15] Zhou J P, Li D, Gu Y S. Chang X R, Zhao C S, Li V S,Qiao L J, Tian Z Z, Fang G D, Song Q S. J Magn MagnMater, 2002; 238: L1
[16] Peng D L, Sumiyama K, Suzuki K. J Alloys Compd, 1997;255: 50
[17] Narayan P B, Kim Y K. IEEE Trans Magn, 1994; 30:3921
[18] Hamrin K, Johansson G, Fahlman A, Nordling C. J PhysChem Solids, 1969; 30: 1835
[19] Herzer G. IEEE Trans Magn, 1990; 26: 1397
[20] Wang H Y, Jiang E Y, Wu P. J Magn Magn Mater, 1998;177-181: 1285
[1] WANG Luning, LIU Lijun, YAN Yu, YANG Kun, LU Lili. Influences of Protein Adsorption on the in vitro Corrosion of Biomedical Metals[J]. 金属学报, 2021, 57(1): 1-15.
[2] TUNG Feng'en;WANG Yuming Institute of Materials Science; Jilin University; Changchun. X-RAY ANALYSIS OF WORK-HARDENING PROCESS FOR POLYCRYSTALLINE а-BRASS DURING UNIAXIAL TENSILE TEST[J]. 金属学报, 1989, 25(2): 82-84.
[3] WANG Jinliang, WANG Chenchong, HUANG Minghao, HU Jun, XU Wei. The Effects and Mechanisms of Pre-Deformation with Low Strain on Temperature-Induced Martensitic Transformation[J]. 金属学报, 2021, 57(5): 575-585.
[4] DU Hegui;LIU Xin Northeast University of Technology; Shenyang. KINETICS OF CARBON COMBUSTION IN PLASMA AIR[J]. 金属学报, 1989, 25(2): 85-88.
[5] . [J]. 金属学报, 2001, 37(1): 42-46 .
[6] . [J]. 金属学报, 1999, 35(3): 320-324 .
[7] . [J]. 金属学报, 2000, 36(1): 72-76 .
[8] . [J]. 金属学报, 1999, 35(3): 330-333 .
[9] . [J]. 金属学报, 1999, 35(3): 334-336 .
[10] . [J]. 金属学报, 2000, 36(6): 647-650 .
[11] . [J]. 金属学报, 2000, 36(6): 655-658 .
[12] No Author. ACTA METALLURGLCA SLNLCA Volume 28 Series A 1992 SUBJECT INDEX[J]. 金属学报, 1992, 28(12): 63-90.
[13] . [J]. 金属学报, 2000, 36(7): 780-784 .
[14] No Author. ACTA METALLURGICA SINICA(JINSHU XUEBAO) Volume 28 1992 AUTHOR INDEX[J]. 金属学报, 1992, 28(12): 71-94.
[15] Хань Яо-вэнь Инсмцмум мемаддов АН КНР;Г.н.Ойкс Московскц цнсмцмум смадц. НЗУЧЕНИЕ ПРОЦЕССОВ ДЕСУЛЬФУРАЦИИ ХНДКОΓО МЕТАЛЛА В ВАКУУМЕ[J]. 金属学报, 1963, 6(2): 98-110.
No Suggested Reading articles found!