Xu Feng-yun. The phase transformation residual stress in granular structure. Acta Metall Sin, 2008, 44(9): 1063-1068 .
|
|
|
Abstract The phase transformation residual stress caused by the volume expansion of transformation from austenite to martensite was calculated by finite element method based on the assumption of specific distribution and shape of martensite island. The effect of residual stress on the macroscopic strain-stress relationship is also discussed. The results show that tension hydrostatic stress exists in ferrite matrix, condensation stress exists in martensite island. The residual stress increases with the increase of the martensite amount, ferrite yield strength and tangent modulus. There is critical martensite amount for ferrite yielding entirely. The residual stress contributes to the continuous yielding of air cooling granular structure steel but effects the yield strength of granular structure little
|
|
Received: 27 November 2007
|
|
|
[1]Fang H S,Bai B Z,Zheng X H,Zheng Y K,Chen X Y, Zhao R F.Acta Metall Sin,1986;22:A283 (方鸿生,白秉哲,郑秀华,郑燕康,陈秀云,赵如发.金属学报,1986:22:A283) [2]Davies R G.Metall Trans,1979;10A:1549 [3]Owen W S.Met Technol,1980;7:1 [4]Bleck W,Phiu-on K.In:Weng Y Q,ed.,Proc The Joint Int Conf of HSLA Steels 2005 and ISUGS(International Symposium on Ultrafine Grained Steels)2005,Beijing: The Chinese Society for Metals,2005:50 [5]Sakaki T,Sugimoto K,Fukuzato T.Acta Metall,1983;31: 1737 [6]Watt D F,Jain M.Scr Metall,1984;18:1379 [7]Pussegoda L N,Tyson W R.Mater Sci Eng,1989;A111: L9 [8]Cheng W Y,Chen Z L,Li E Q,Chen Q K,Ma M Y.Phys Exam Test,1996;(4):1 (陈文义,陈智力,李恩勤,陈启宽,马茂元.物理测试,1996;(4):1) [9]Peng Y L,Tan S H,Zhang L,He S L,Ma M Y,Wang Y J.Hot Work Technol,1997;(2):6 (彭延玲,谭松华,张磊,何松林,马茂元,王艺坚.热加工工艺,1997;(2):6 [10]Hüper T,Endo S,Ishikawa N,Osawa K.ISIJ Int,1999; 39:288 [11]Liedl U,Traint S,Werner E A.Comput Mater Sci,2002; 25:122 [12]Ankem S,Margolin H.Metall Trans,1982;13A:595 [13]Li Z H,Gu H C.J Xi'an Jiaotong Univ,1990;24(2):23 (李中华,顾海澄.西安交通大学学报,1990;24(2):23 [14]Socrate S,Boyce M C.J Mech Phys Solids,2000;48:233 [15]Al-Abbasi F M,Nemes J A.Int J Mech Sci,2003;45: 1449 [16]Al-Abbasi F M,Nemes J A.Int d Solid Struct,2003;40: 3379 [17]Tomota Y,Kuroki K,Mori T,Tamura I.Mater Sci Eng, 1976;24:85 [18]Maiya S.Produce and Correspondin9 Policy of Residual Stress.Tokyo:Yokendo,1975 (米谷茂.残余应力の发生と对策.东京:养贤堂,1975) [19]Kang F Y,Tang N Y,Liu X Y.J Mech Strength,1991; 13(1):22 (康飞宇,唐迺泳,刘秀瀛.机械强度,1991;13(1):22) |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|