An optimization algorithm and its application for predicting elemental concentrations of sublattices of γ' phase in Ni base superalloys
YAN Guangzong; PENG Zhifang
Department of Materials Engineering; College of Power and Mechanical Engineering; Wuhan University; Wuhan 430072
Cite this article:
YAN Guangzong; PENG Zhifang. An optimization algorithm and its application for predicting elemental concentrations of sublattices of γ' phase in Ni base superalloys. Acta Metall Sin, 2005, 41(3): 251-254 .
Abstract The effects of mismatch in atomic size and electronegativity of
alloying elements on the elemental concentration of sublattices
of γ' phase in Ni base superalloys were
investigated. The mathematic model of optimizations was
established to predict the elemental
concentration of sublattices of γ'
phase. Ranges of the selected values of concentration variables
were determined by use of the iterative and substitutional method.
Based on chemical compositions of the γ' phase,
the elemental content at the Ni and Al sites in the γ'phase can be calculated with
the layered multi-objective optimization algorithm with tolerance.
Using the reported data on both
the chemical compositions and the lattice parameters of γ'
phase, a comparison between the predicted and the reported values
of lattice parameters was made through the application of the
predicted values of the elemental concentrations of the γ'sublattices to verify the feasibility and the
accuracy of the present method.
[1] Peng Z F, Liu P. Acta Matall Sin, 2004; 40: 569 (彭志方,刘攀,金属学报,2004;40:569) [2] Hu S G, Shi B C. Principles of Optimization Algorithms. Wuhan: Huazhong University of Science and Technology, 2000: 5 (胡适耕,施保昌,最优化原理.武汉:华中理工大学出版社, 2000:5) [3] Pan J S, Tong J M. Basis of Material Science. Beijing: Tsinghua University Press, 1998: 90 (潘金生,仝健民.材料科学基础.北京:清华大学出版社, 1998:90) [4] Xiao J M, Zhu F W. Energetics of Materials. Shanghai: Shanghai Science and Technology Press, 1999: 266 (肖纪美,朱逢吾.材料能量学.上海:上海科学技术出版社, 1999:266) [5] Xie K X, Han L X, Lin Y L. Method of Optimization Algorithms. Tianjin: Tianjin University Press, 1997: 1 (解可新,韩立兴,林友联.最优化方法.天津:天津大学出版 社,1997:1) [6] Caron P, Khan T. Mater Sci Eng, 1983; 61: 173 [7] Kuhn H A, Biermann H, Ungar T, Mughrabi H. Acta Met- all Mater, 1991; 39: 2783 [8] Nathal M V, Ebert L J. Metall Trans, 1985; 16A: 1849 [9] Harf F H. Metall Trans, 1985; 16A: 993 [10] Narayan V. University of Cambridge, 1999, In: http:// www.msm.cam.ac.uk/map/data/neural/lattmisfit-b.html [11] Bruckner U, Epishin A, Link T, Dressel K. Mater Sci Eng, 1998; A247: 23 [12] Copland E H, Jacobson N S, Ritzert F J. NASA TM-2001-210897, 2001