Cite this article:
. . Acta Metall Sin, 2002, 38(8): 881-884 .
|
|
|
|
|
Received: 18 December 2001
|
|
|
[1] Liao J H. Laser Technol, 1997; 21: 164(廖健宏.激光技术.1997;21:164) [2] Radaj D, translated by Xiong D J et al. Heat Effects ofWelding: Temperature Field, Residual Stress, Distortion.Beijing: Machinery Industry Press, 1997: 47(Radai D 著,熊第京等译.焊接热效应——温度场、残余应力、变形.北京:机械工业出版社,1997:47) [3] Gianoulakis B E, Burchett S N. DE 95006314, 1995 [4] Schrank M. DE 91016454, 1991 [5] Carmignani C, Mares R, Toselli G. Comput Methods ApplMech Engrg, 1999; 179: 197 [6] Zhao H, Debroy T. Metall Mater Trans, 2001; 32B: 163 [7] Lindgren L E, Karlsson L. Int J Numer Methods Engrg,1988; 25: 635 [8] Tekriwal P, Mazumder P. J Engrg Mater Technol, 1991;113: 336 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|