Experimental Study on Mold Oscillation-Less Continuous Casting Process Under High Frequency Amplitude-Modulated Magnetic Field
LEI Zuosheng; REN Zhongming; YAN Yonggang; DENG Kang
Cite this article: 

LEI Zuosheng; REN Zhongming; YAN Yonggang; DENG Kang. Experimental Study on Mold Oscillation-Less Continuous Casting Process Under High Frequency Amplitude-Modulated Magnetic Field. Acta Metall Sin, 2004, 40(9): 995-999 .

Download:  PDF(11794KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  A high frequency amplitude-modulated magnetic field (AMMF) generator that can produce rectangle, triangle and sine waves has been invented, and the magnetic field inducted in the mold by the generator was measured. The amplitude-modulated magnetic field has been applied in mold oscillation-less electromagnetic continuous casting (MOLECC) process, the experiment results show that under rectangle, triangle and sine wave AMMF, when the modulated wave frequency is a little less then the intrinsic frequency of the experimental system the intermittent contacting distance is the greatest, the mold flux lubricating is the best, the continuous casting withdraw resistance is the least and the surface quality of billets is better relatively. Among the three wave types, the sine wave is better than the rectangle and triangle waves for deducing the withdraw resistance and improving the billets surface quality.
Key words:  electromagnetic continuous casting      high frequency amplitude-modulated magnetic field      
Received:  28 August 2003     
ZTFLH:  TG249.7  
  TG111.4  

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y2004/V40/I9/995

[1] Asai S. Tetsu Hagane, 1989; 75: 32(浅井滋生.铁 钢,1989;75:32)
[2] Ren Z M, Dong H F, Deng K. ISIJ Int, 2001; 41: 981
[3] Li T J, Sassa K, Asai S. ISIJ Int, 1996; 36: 410
[4] Zhou Y M, Sassa K, Asai S. Tetsu Hagane, 1999; 85: 460(周月明,佐佐健介,浅井滋生.铁 钢,1999;85:460)
[5] Su Z J, Iwai K, Asai S. CAMP-ISIJ, 1998; 11: 132 (苏志坚,岩井一彦,浅井滋生.材料 ,1998;11:132)
[6] Su Z J, Iwai K, Asai S. ISIJ Int, 1999; 39: 1224
[7] Zhou Y M, Sassa K, Asai S. Acta Metall Sin, 2001; 37:777(周月明,佐佐健介,浅井滋生.金属学报, 2001;37:777)
[8] Lei Z S, Ren Z M, Deng K. Chin J Nonferrous Met, 2002; 12 (Suppl.1) : 30(雷作胜,任忠鸣,邓康.中国有色金属学报,2002;12(增刊1) :30)
[9] Dong H F, Ren Z M, Zhong Y B, Deng K. J Iron Steel Res, 1998; 10: 5(董华峰,任忠鸣,钟云波,邓康.钢铁研究学报,1998;10:5)
[10] Sassa K, Li T J, Asai S. Tetsu Hagane, 1993, 79: 1075(佐佐健介,李廷举,浅井滋生.铁 钢, 1993;79:1075)
[11] Zhou Y M, Sassa K, Asai S. Acta Metall Sin, 2001; 37: 772(周月明,佐佐健介,浅井滋生.金属学报, 2001;37:772)
[12] Ye J T, Liu Z R, Xu S X, W Z. Hydrodynamics. Shanghai: Fudan University Press, 1989: 345(叶敬棠,柳兆荣,许世雄,吴正.流体力学.上海:复旦大学出版社, 1989:345)
[13] Li T J, Sassa K, Asai S. Acta Metall Sin, 1997; 33: 971(李廷举,佐佐健介,浅井滋生.金属学报, 1997;33:971)
[14] Chen F, Duan Z L, Wang W A. Experiments of Material Mechanics. Wuhan: Huazhong University of Science & Technology Press, 1999: 133(陈锋,段自力,王文安.材料力学实验.武汉:华中理工大学出版社, 1999:133)
[15] Zhang X Y, Qi B M, Zhu X L. Applied Chemic Handbook. Beijing: National Defence Industry Press, 1986: 322(张向宇,戚保民,朱鑫林.实用化学手册.北京:国防工业出版社, 1986:322)
[1] Bai-Gang JIN. PENETRATION OF MAGNETIC FIELD IN TWO-STAGE SLITLESS MOLD FOR SOFT-CONTACT ELECTROMAGNETIC CONTINUOUS CASTING[J]. 金属学报, 2008, 44(7): 883-886 .
[2] Bai-Gang JIN; Qiang WANG. ELECTROMAGNETIC FIELD DISTRIBUTION IN TWO-STAGE SLITLESS SOFT CONTACT ELECTROMAGNETIC CONTINUOUS CASTING MOLD[J]. 金属学报, 2007, 43(9): 999-1003 .
[3] Bai-Gang JIN. NUMERICAL SIMULATION OF ELECTROMAGNETISM PARAMETERS AND STRUCTURE PARAMETERS IN TWO-STAGE SLIT-LESS MOLD[J]. 金属学报, 2007, 43(4): 427-432 .
[4] LEI Zuosheng; REN Zhongming; YAN Yonggang; DENG Kang. Mold Flux Channel Dynamic Pressure in Electromagnetic Continuous Casting[J]. 金属学报, 2004, 40(5): 546-550 .
No Suggested Reading articles found!