Abstract A high frequency amplitude-modulated magnetic field (AMMF) generator
that can produce rectangle, triangle and sine waves has been
invented, and the magnetic field inducted in the mold by the
generator was measured. The amplitude-modulated magnetic
field has been applied in mold oscillation-less
electromagnetic continuous casting (MOLECC) process,
the experiment results show that
under rectangle, triangle and sine
wave AMMF, when the modulated wave frequency is a little less
then the intrinsic frequency of the experimental system the
intermittent contacting distance is the greatest,
the mold flux lubricating is the best, the continuous
casting withdraw resistance is the least and the surface
quality of billets is better relatively. Among
the three wave types, the sine wave is better than
the rectangle and triangle waves for deducing
the withdraw resistance and improving the billets surface quality.
|
|
Received: 28 August 2003
|
|
|
[1] Asai S. Tetsu Hagane, 1989; 75: 32(浅井滋生.铁 钢,1989;75:32) [2] Ren Z M, Dong H F, Deng K. ISIJ Int, 2001; 41: 981 [3] Li T J, Sassa K, Asai S. ISIJ Int, 1996; 36: 410 [4] Zhou Y M, Sassa K, Asai S. Tetsu Hagane, 1999; 85: 460(周月明,佐佐健介,浅井滋生.铁 钢,1999;85:460) [5] Su Z J, Iwai K, Asai S. CAMP-ISIJ, 1998; 11: 132 (苏志坚,岩井一彦,浅井滋生.材料 ,1998;11:132) [6] Su Z J, Iwai K, Asai S. ISIJ Int, 1999; 39: 1224 [7] Zhou Y M, Sassa K, Asai S. Acta Metall Sin, 2001; 37:777(周月明,佐佐健介,浅井滋生.金属学报, 2001;37:777) [8] Lei Z S, Ren Z M, Deng K. Chin J Nonferrous Met, 2002; 12 (Suppl.1) : 30(雷作胜,任忠鸣,邓康.中国有色金属学报,2002;12(增刊1) :30) [9] Dong H F, Ren Z M, Zhong Y B, Deng K. J Iron Steel Res, 1998; 10: 5(董华峰,任忠鸣,钟云波,邓康.钢铁研究学报,1998;10:5) [10] Sassa K, Li T J, Asai S. Tetsu Hagane, 1993, 79: 1075(佐佐健介,李廷举,浅井滋生.铁 钢, 1993;79:1075) [11] Zhou Y M, Sassa K, Asai S. Acta Metall Sin, 2001; 37: 772(周月明,佐佐健介,浅井滋生.金属学报, 2001;37:772) [12] Ye J T, Liu Z R, Xu S X, W Z. Hydrodynamics. Shanghai: Fudan University Press, 1989: 345(叶敬棠,柳兆荣,许世雄,吴正.流体力学.上海:复旦大学出版社, 1989:345) [13] Li T J, Sassa K, Asai S. Acta Metall Sin, 1997; 33: 971(李廷举,佐佐健介,浅井滋生.金属学报, 1997;33:971) [14] Chen F, Duan Z L, Wang W A. Experiments of Material Mechanics. Wuhan: Huazhong University of Science & Technology Press, 1999: 133(陈锋,段自力,王文安.材料力学实验.武汉:华中理工大学出版社, 1999:133) [15] Zhang X Y, Qi B M, Zhu X L. Applied Chemic Handbook. Beijing: National Defence Industry Press, 1986: 322(张向宇,戚保民,朱鑫林.实用化学手册.北京:国防工业出版社, 1986:322) |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|